Materials / Compare

Drywall vs. Titanium Ti-6Al-4V

Compare Drywall vs. Titanium Ti-6Al-4V strength, stiffness, weight and thermal properties.

Change either side
DrywallNatural
Titanium Ti-6Al-4VWrought
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)885MPasourcetypical, plate (>0.187 in), annealed, 0.2% offset
Ultimate tensile strength1–2MPasourceambient range reported in review (Australian studies)940MPasourcetypical, plate, annealed
Compressive strength2.4MPasourcetypical, 70 F / 50% RHnot sourced
Elongation at breaknot sourced16%sourcetypical, in 2 in., plate annealed
Young's modulus (stiffness)1–2GPasourceambient range reported in review (Australian studies)107–122GPasourcetypical range, 20 °C
Densitynot sourced4,430kg/m³sourcenominal
Strength to weightnot sourced200kN·m/kg
Stiffness to weightnot sourced25.8MN·m/kg
Poisson's rationot sourced0.342sourcemean of TIMET measurements
Shear modulusnot sourced42.7GPa
Bulk modulusnot sourced121GPa
Speed of soundnot sourced5,084m/s
Thermal
Thermal conductivitynot sourced6.6W/m·Ksourcetypical, 20 °C, mill annealed
Thermal expansion16.7µm/m·Ksourcetypical, unrestrained, 3.3-32 C9µm/m·Ksourcetypical, mean 0-100 °C
100 mm part over a 50 °C swing83.5µm growth45µm growth1.86x less
Specific heat1,090J/kg·Ksourcetypical (from ASHRAE Handbook of Fundamentals, per GA)580J/kg·Ksourcetypical, 20 °C
Heats up and cools (diffusivity)not sourced2.57mm²/s
Thermal shock resistancenot sourced3,730W/m
Melting pointnot sourced1,630–1,650°Csourcemelting range
Max service temperature52°Csourcemanufacturer sustained-exposure limit400°Csourceupper recommended use temperature
Values for1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittalTIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Drywall stronger than Titanium Ti-6Al-4V?

Titanium Ti-6Al-4V is stronger: its yield strength is 885 MPa against tensile strength 1.5 MPa for Drywall (590x).

Which is stiffer, Drywall or Titanium Ti-6Al-4V?

Titanium Ti-6Al-4V is stiffer: Young's modulus 115 GPa against 1.5 GPa for Drywall, so the same part in Titanium Ti-6Al-4V deflects less under the same load.

Which expands less with temperature?

Titanium Ti-6Al-4V expands less: 9 µm/m·K against 16.7 µm/m·K for Drywall.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Brass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelTitanium Ti-6Al-4V
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Brass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickTitanium Ti-6Al-4V
Strength against density