Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
TIMETAL 6-4 Data SheetTIMETarchived copyTitanium Ti-6Al-4V · Young's modulus (stiffness): typical range, 20 °CTitanium Ti-6Al-4V · Thermal conductivity: typical, 20 °C, mill annealedTitanium Ti-6Al-4V · Thermal expansion: typical, mean 0-100 °CTitanium Ti-6Al-4V · Specific heat: typical, 20 °C
4
Luran S 777K (ASA) Product Data SheetINEOS StyrolutionFDM ASA · Thermal conductivity: base material: INEOS Styrolution Luran S 777K injection-molding ASA, typicalFDM ASA · Thermal expansion: base material: INEOS Styrolution Luran S 777K injection-molding ASA, range
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM ASA is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is FDM ASA stronger than Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V is stronger: its yield strength is 885 MPa against tensile strength 37 MPa for FDM ASA (23.9x).
Which is lighter, FDM ASA or Titanium Ti-6Al-4V?
FDM ASA is lighter: 1,050 kg/m³ against 4,430 kg/m³ for Titanium Ti-6Al-4V.
Which is stiffer, FDM ASA or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V is stiffer: Young's modulus 115 GPa against 2.45 GPa for FDM ASA, so the same part in Titanium Ti-6Al-4V deflects less under the same load.
Which is lighter for the same job, FDM ASA or Titanium Ti-6Al-4V?
For the same stiffness or strength: FDM ASA is lighter for a stiff panel or plate; Titanium Ti-6Al-4V is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam, strong panel or plate.
Part that must be
FDM ASA
Titanium Ti-6Al-4V
Stiff rod or tie (tension)
11.1x heavier
lighter
Stiff beam (bending)
1.62x heavier
lighter
Stiff panel or plate
lighter
17% heavier
Strong rod or tie
5.67x heavier
lighter
Strong beam
1.97x heavier
lighter
Strong panel or plate
16% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, FDM ASA or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V stretches further before it breaks: 16% elongation at break against 9.2% for FDM ASA.
Thermal
Which conducts heat better, FDM ASA or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V conducts heat better: 6.6 W/m·K against 0.17 W/m·K for FDM ASA.
Which expands less with temperature?
Titanium Ti-6Al-4V expands less: 9 µm/m·K against 95 µm/m·K for FDM ASA.