Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
BASF Forward AM (BASF 3D Printing Solutions) Ultrafuse HiPS, TDS v2.2 (13.11.2019), printed specimens, XY 'Flat'. Specimen print settings are not stated; recommended processing on the sheet: nozzle 240-260 °C, bed 100-120 °C, 40-80 mm/s. Product is discontinued (Forward AM product page) but the TDS is still served by Forward AM.
Wood
Northern red oak (Quercus rubra), clear straight-grained specimens at 12% MC, parallel to grain unless stated; USDA FPL Wood Handbook FPL-GTR-282 (2021) Ch. 4 and Ch. 5
Wood Handbook (FPL-GTR-282), Chapter 5: Mechanical Properties of WoodUSDA Forest Products LaboratoryWood · Ultimate tensile strength: modulus of rupture (no direct tensile value)Wood · Compressive strength: compression parallel to grain (maximum crushing strength), 12% MCWood · Flexural strength: modulus of rupture (static bending), 12% MCWood · Young's modulus (stiffness): bending MOE, parallel to grainWood · Poisson's ratio: mu_LR (red oak group, ~12% MC)
3
Technical Note 218: Weights of Various Woods Grown in the United States (1953)USDA Forest Products LaboratoryWood · Density: average weight of clear wood at 8% and 15% moisture content
Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryWood · Thermal conductivity: across grain, 12% MC (Table 4-7, approximate)Wood · Thermal expansion: parallel to grain, ovendry wood, range across speciesWood · Specific heat: solid wood (all species), 12% MC, 27 C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM HIPS is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is FDM HIPS stronger than Wood?
Wood is stronger: its tensile strength is 99 MPa against 18.4 MPa for FDM HIPS (5.38x).
Which is lighter, FDM HIPS or Wood?
Wood is lighter: 692 kg/m³ against 1,023 kg/m³ for FDM HIPS.
Which is stiffer, FDM HIPS or Wood?
Wood is stiffer: Young's modulus 12.5 GPa against 1.59 GPa for FDM HIPS, so the same part in Wood deflects less under the same load.
Which is lighter for the same job, FDM HIPS or Wood?
For the same stiffness or strength: Wood is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
FDM HIPS
Wood
Stiff rod or tie (tension)
11.6x heavier
lighter
Stiff beam (bending)
4.15x heavier
lighter
Stiff panel or plate
2.94x heavier
lighter
Strong rod or tie
7.96x heavier
lighter
Strong beam
4.54x heavier
lighter
Strong panel or plate
3.43x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, FDM HIPS or Wood?
Wood conducts heat better: 0.18 W/m·K against 0.17 W/m·K for FDM HIPS.
Which expands less with temperature?
Wood expands less: 3.8 µm/m·K against 80 µm/m·K for FDM HIPS.