Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Sources3 documents: LyondellBasell, Pilkington North America, INEOS Olefins & Polymers USA
Glass
Annealed soda-lime-silica float glass, Pilkington North America Technical Bulletin ATS-129 (04/2025)
Plastic HDPE
LyondellBasell Hostalen 23050 B high density polyethylene, typical ISO values
1
Hostalen 23050 B Product DataLyondellBasellPlastic HDPE · Yield strength: typical, tensile stress at yield 23 °C, 50 mm/min ISO 527Plastic HDPE · Young's modulus (stiffness): typical, tensile modulus 23 °C ISO 527Plastic HDPE · Density: typical, ISO 1183
2
Technical Bulletin ATS-129: Properties of Soda-Lime Silica Float Glass (2025)Pilkington North Americaarchived copyGlass · Ultimate tensile strength: typical mean surface tensile stress at fracture (MOR), 60 s load, weathered, 50% breakage probabilityGlass · Flexural strength: mean MOR (same value as tensile)Glass · Young's modulus (stiffness): typicalGlass · Density: typicalGlass · Poisson's ratio: typicalGlass · Thermal conductivity: typical at 75 FGlass · Thermal expansion: typical, 75-575 FGlass · Specific heat: typical at 75 FGlass · Max service temperature: strain point (ASTM C336) - stress-relaxation onset, not a rated service limit
3
Typical Engineering Properties of High Density PolyethyleneINEOS Olefins & Polymers USAarchived copyPlastic HDPE · Poisson's ratio: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal conductivity: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal expansion: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Specific heat: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Glass stronger than Plastic HDPE?
Glass is stronger: its tensile strength is 41 MPa against yield strength 24 MPa for Plastic HDPE (1.71x).
Which is lighter, Glass or Plastic HDPE?
Plastic HDPE is lighter: 950 kg/m³ against 2,500 kg/m³ for Glass.
Which is stiffer, Glass or Plastic HDPE?
Glass is stiffer: Young's modulus 72 GPa against 0.9 GPa for Plastic HDPE, so the same part in Glass deflects less under the same load.
Which is lighter for the same job, Glass or Plastic HDPE?
For the same stiffness or strength: Glass is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Plastic HDPE is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Glass
Plastic HDPE
Stiff rod or tie (tension)
lighter
30.4x heavier
Stiff beam (bending)
lighter
3.4x heavier
Stiff panel or plate
lighter
1.64x heavier
Strong rod or tie
1.54x heavier
lighter
Strong beam
1.84x heavier
lighter
Strong panel or plate
2.01x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Glass or Plastic HDPE?
Glass conducts heat better: 0.937 W/m·K against 0.445 W/m·K for Plastic HDPE.
Which expands less with temperature?
Glass expands less: 8.3 µm/m·K against 120 µm/m·K for Plastic HDPE.