Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Sources3 documents: Celanese, Pilkington North America
Glass
Annealed soda-lime-silica float glass, Pilkington North America Technical Bulletin ATS-129 (04/2025)
Plastic UHMWPE
Celanese GUR 4120 (avg. molecular weight 4.7x10^6 g/mol), typical values on compression-molded specimens; CTE and thermal conductivity from Celanese's generic UHMWPE guide (grade not named)
1
GUR UHMW-PE Overview (GUR-015)CelanesePlastic UHMWPE · Yield strength: typical, tensile stress at yield ISO 527, 50 mm/minPlastic UHMWPE · Ultimate tensile strength: typical, tensile stress at break ISO 527, 50 mm/minPlastic UHMWPE · Elongation at break: typical, nominal elongation at break ISO 527Plastic UHMWPE · Young's modulus (stiffness): typical, tensile modulus ISO 527, 1 mm/minPlastic UHMWPE · Density: typicalPlastic UHMWPE · Melting point: DSC 10 K/minPlastic UHMWPE · Max service temperature: recommended max constant operating temperature
2
Technical Bulletin ATS-129: Properties of Soda-Lime Silica Float Glass (2025)Pilkington North Americaarchived copyGlass · Ultimate tensile strength: typical mean surface tensile stress at fracture (MOR), 60 s load, weathered, 50% breakage probabilityGlass · Flexural strength: mean MOR (same value as tensile)Glass · Young's modulus (stiffness): typicalGlass · Density: typicalGlass · Poisson's ratio: typicalGlass · Thermal conductivity: typical at 75 FGlass · Thermal expansion: typical, 75-575 FGlass · Specific heat: typical at 75 FGlass · Max service temperature: strain point (ASTM C336) - stress-relaxation onset, not a rated service limit
3
GUR UHMW-PE Polymer Guide (GUR-003)Celanesearchived copyPlastic UHMWPE · Thermal conductivity: typical, unfilled (narrative value, generic Celanese UHMWPE)Plastic UHMWPE · Thermal expansion: typical, 20 to 100 °C (generic Celanese UHMWPE)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Glass stronger than Plastic UHMWPE?
Glass is stronger: its tensile strength is 41 MPa against yield strength 20 MPa for Plastic UHMWPE (2.05x).
Which is lighter, Glass or Plastic UHMWPE?
Plastic UHMWPE is lighter: 930 kg/m³ against 2,500 kg/m³ for Glass.
Which is stiffer, Glass or Plastic UHMWPE?
Glass is stiffer: Young's modulus 72 GPa against 0.66 GPa for Plastic UHMWPE, so the same part in Glass deflects less under the same load.
Which is lighter for the same job, Glass or Plastic UHMWPE?
For the same stiffness or strength: Glass is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Plastic UHMWPE is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Glass
Plastic UHMWPE
Stiff rod or tie (tension)
lighter
40.6x heavier
Stiff beam (bending)
lighter
3.89x heavier
Stiff panel or plate
lighter
1.78x heavier
Strong rod or tie
31% heavier
lighter
Strong beam
1.67x heavier
lighter
Strong panel or plate
1.88x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Glass or Plastic UHMWPE?
Glass conducts heat better: 0.937 W/m·K against 0.4 W/m·K for Plastic UHMWPE.
Which expands less with temperature?
Glass expands less: 8.3 µm/m·K against 200 µm/m·K for Plastic UHMWPE.