Materials / Compare

Glass vs. Stainless 316

Compare Glass vs. Stainless 316 strength, stiffness, weight and thermal properties.

Change either side
GlassNatural
Stainless 316Wrought
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)265MPasourcetypical (representative), annealed 1.0 mm sheet
Ultimate tensile strength41MPasourcetypical mean surface tensile stress at fracture (MOR), 60 s load, weathered, 50% breakage probability583MPasourcetypical (representative), annealed 1.0 mm sheet
Flexural strength41MPasourcemean MOR (same value as tensile)not sourced
Elongation at breaknot sourced61%sourcetypical (representative), annealed, in 2 in. (51 mm)
Young's modulus (stiffness)72GPasourcetypical200GPasourcetypical, in tension
Density2,500kg/m³sourcetypical3.21x lighter8,027kg/m³sourcetypical
Strength to weight16.4kN·m/kg33kN·m/kg2.01x higher
Stiffness to weight28.8MN·m/kg16% higher24.9MN·m/kg
Poisson's ratio0.22sourcetypical0.3sourcedesign value (structural stainless steels)
Shear modulus29.5GPa76.9GPa2.61x stiffer in shear
Bulk modulus42.9GPa167GPa
Speed of sound5,367m/s4,992m/s
Thermal
Thermal conductivity0.937W/m·Ksourcetypical at 75 F14.6W/m·Ksource20–100 °C
Thermal expansion8.3µm/m·Ksourcetypical, 75-575 F16.5µm/m·Ksourcemean, 20–100 °C
100 mm part over a 50 °C swing41.5µm growth1.99x less82.5µm growth
Specific heat880J/kg·Ksourcetypical at 75 F450J/kg·Ksourceat 20 °C
Heats up and cools (diffusivity)0.426mm²/s4.04mm²/s9.49x faster
Thermal shock resistance50.1W/m821W/m16.4x more resistant
Melting pointnot sourced1,390–1,440°Csourcemelting range
Max service temperature511°Csourcestrain point (ASTM C336) - stress-relaxation onset, not a rated service limit871–899°Csourceoxidation (scaling) limit in air
Values forAnnealed soda-lime-silica float glass, Pilkington North America Technical Bulletin ATS-129 (04/2025)ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Glass stronger than Stainless 316?

Stainless 316 is stronger: its yield strength is 265 MPa against tensile strength 41 MPa for Glass (6.46x).

Which is lighter, Glass or Stainless 316?

Glass is lighter: 2,500 kg/m³ against 8,027 kg/m³ for Stainless 316.

Which is stiffer, Glass or Stainless 316?

Stainless 316 is stiffer: Young's modulus 200 GPa against 72 GPa for Glass, so the same part in Stainless 316 deflects less under the same load.

Which is lighter for the same job, Glass or Stainless 316?

For the same stiffness or strength: Glass is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong panel or plate; Stainless 316 is lighter for a strong rod or tie, strong beam.

Part that must beGlassStainless 316
Stiff rod or tie (tension)lighter16% heavier
Stiff beam (bending)lighter1.93x heavier
Stiff panel or platelighter2.28x heavier
Strong rod or tie2.01x heavierlighter
Strong beam8% heavierlighter
Strong panel or platelighter26% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Glass or Stainless 316?

Stainless 316 conducts heat better: 14.6 W/m·K against 0.937 W/m·K for Glass.

Which expands less with temperature?

Glass expands less: 8.3 µm/m·K against 16.5 µm/m·K for Stainless 316.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Steel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelGlassStainless 316
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Steel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickGlassStainless 316
Strength against density