Materials / Compare

Glass vs. Stainless Steel 304

Compare Glass vs. Stainless Steel 304 strength, stiffness, weight and thermal properties.

GlassNatural
Stainless Steel 304Wrought
MechanicalGlassStainless Steel 304
Yield strengthnone (brittle)241MPa1
Ultimate tensile strength41MPa2586MPa114.3x stronger
Flexural strengthmean MOR41MPa2not sourced
Elongation at breaknone (brittle)55%1
Young's modulus (stiffness)72GPa2193GPa12.68x stiffer
Density2,500kg/m³23.21x lighter8,030kg/m³1
Strength to weight16.4kN·m/kg30kN·m/kg1.83x higher
Stiffness to weight28.8MN·m/kg20% higher24MN·m/kg
Poisson's ratio0.222design value0.33
Shear modulus29.5GPa74.2GPa2.52x stiffer in shear
Bulk modulus42.9GPa161GPa3.75x higher
Speed of sound5,367m/s9% faster4,903m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30GlassStainless Steel 304
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30GlassStainless Steel 304
Strength against densityHigher and further left: stronger for its weight
ThermalGlassStainless Steel 304
Thermal conductivity0.937W/m·K2at 100 °C16.2W/m·K117.3x more heat through a fin
Thermal expansion8.3µm/m·K22.04x lessmean16.9µm/m·K1
100 mm part over a 50 °C swing41.5µm growth2.04x less84.5µm growth
Specific heat880J/kg·K21.76x highermean500J/kg·K1
Heats up and cools (diffusivity)0.426mm²/s4.03mm²/s9.47x faster
Thermal shock resistance50.1W/m838W/m16.7x more resistant
Melting pointnot sourcedmelting range1,399–1,454°C1
Max service temperaturestrain point511°C2continuous899°C1
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30GlassStainless Steel 304
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200Steel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30GlassStainless Steel 304
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Cleveland-Cliffs, Pilkington North America, Steel Construction Institute
Glass
Annealed soda-lime-silica float glass, Pilkington North America Technical Bulletin ATS-129 (04/2025)
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
  1. 1
    304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
  2. 2
    Technical Bulletin ATS-129: Properties of Soda-Lime Silica Float Glass (2025)Pilkington North Americaarchived copyGlass · Ultimate tensile strength: typical mean surface tensile stress at fracture (MOR), 60 s load, weathered, 50% breakage probabilityGlass · Flexural strength: mean MOR (same value as tensile)Glass · Young's modulus (stiffness): typicalGlass · Density: typicalGlass · Poisson's ratio: typicalGlass · Thermal conductivity: typical at 75 FGlass · Thermal expansion: typical, 75-575 FGlass · Specific heat: typical at 75 FGlass · Max service temperature: strain point (ASTM C336) - stress-relaxation onset, not a rated service limit
  3. 3
    Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Glass stronger than Stainless Steel 304?

Stainless Steel 304 is stronger: its yield strength is 241 MPa against tensile strength 41 MPa for Glass (5.88x).

Which is lighter, Glass or Stainless Steel 304?

Glass is lighter: 2,500 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.

Which is stiffer, Glass or Stainless Steel 304?

Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 72 GPa for Glass, so the same part in Stainless Steel 304 deflects less under the same load.

Which is lighter for the same job, Glass or Stainless Steel 304?

For the same stiffness or strength: Glass is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong panel or plate; Stainless Steel 304 is lighter for a strong rod or tie, strong beam.

Part that must beGlassStainless Steel 304
Stiff rod or tie (tension)lighter20% heavier
Stiff beam (bending)lighter1.96x heavier
Stiff panel or platelighter2.31x heavier
Strong rod or tie1.83x heavierlighter
Strong beam1% heavierlighter
Strong panel or platelighter32% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Glass or Stainless Steel 304?

Stainless Steel 304 conducts heat better: 16.2 W/m·K against 0.937 W/m·K for Glass.

Which expands less with temperature?

Glass expands less: 8.3 µm/m·K against 16.9 µm/m·K for Stainless Steel 304.

Related comparisons