Glass
Annealed soda-lime-silica float glass, Pilkington North America Technical Bulletin ATS-129 (04/2025)
Stainless Steel 316
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
1
ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
2
Technical Bulletin ATS-129: Properties of Soda-Lime Silica Float Glass (2025)Pilkington North Americaarchived copyGlass · Ultimate tensile strength: typical mean surface tensile stress at fracture (MOR), 60 s load, weathered, 50% breakage probabilityGlass · Flexural strength: mean MOR (same value as tensile)Glass · Young's modulus (stiffness): typicalGlass · Density: typicalGlass · Poisson's ratio: typicalGlass · Thermal conductivity: typical at 75 FGlass · Thermal expansion: typical, 75-575 FGlass · Specific heat: typical at 75 FGlass · Max service temperature: strain point (ASTM C336) - stress-relaxation onset, not a rated service limit
3
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Glass stronger than Stainless Steel 316?
Stainless Steel 316 is stronger: its yield strength is 265 MPa against tensile strength 41 MPa for Glass (6.46x).
Which is lighter, Glass or Stainless Steel 316?
Glass is lighter: 2,500 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.
Which is stiffer, Glass or Stainless Steel 316?
Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 72 GPa for Glass, so the same part in Stainless Steel 316 deflects less under the same load.
Which is lighter for the same job, Glass or Stainless Steel 316?
For the same stiffness or strength: Glass is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong panel or plate; Stainless Steel 316 is lighter for a strong rod or tie, strong beam.
Part that must be
Glass
Stainless Steel 316
Stiff rod or tie (tension)
lighter
16% heavier
Stiff beam (bending)
lighter
1.93x heavier
Stiff panel or plate
lighter
2.28x heavier
Strong rod or tie
2.01x heavier
lighter
Strong beam
8% heavier
lighter
Strong panel or plate
lighter
26% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Glass or Stainless Steel 316?
Stainless Steel 316 conducts heat better: 14.6 W/m·K against 0.937 W/m·K for Glass.
Which expands less with temperature?
Glass expands less: 8.3 µm/m·K against 16.5 µm/m·K for Stainless Steel 316.