Materials / Compare

Iron vs. Plastic PMMA

Compare Iron vs. Plastic PMMA strength, stiffness, weight and thermal properties.

IronWrought
Plastic PMMABulk polymer (molded or machined)
MechanicalIronPlastic PMMA
Yield strength186MPa1not given (tensile used)
Ultimate tensile strength290MPa13.63x stronger80MPa2
Compressive strengthnot sourced110MPa2
Flexural strengthnot sourced115MPa2
Elongation at break38%16.91x more ductile5.5%2
Young's modulus (stiffness)207GPa162.7x stiffer3.3GPa2
Density7,860kg/m³11,190kg/m³26.61x lighter
Strength to weight23.7kN·m/kg67.2kN·m/kg2.84x higher
Stiffness to weight26.3MN·m/kg9.5x higher2.77MN·m/kg
Poisson's ratio0.28230.372
Shear modulus80.7GPa67x stiffer in shear1.2GPa
Bulk modulus158GPa37.4x higher4.23GPa
Speed of sound5,132m/s3.08x faster1,665m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PMMA
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PMMA
Strength against densityHigher and further left: stronger for its weight
ThermalIronPlastic PMMA
Thermal conductivity73.2W/m·K1385x more heat through a fin0.19W/m·K2
Thermal expansionmean13.7µm/m·K15.11x less0-50 °C70µm/m·K2
100 mm part over a 50 °C swing68.5µm growth5.11x less350µm growth
Specific heat450J/kg·K11,470J/kg·K23.27x higher
Heats up and cools (diffusivity)20.7mm²/s191x faster0.109mm²/s
Thermal shock resistance3,447W/m83.2x more resistant41.5W/m
Melting point1,532°C1not sourced
Max service temperaturenot sourced80°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PMMA
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PMMA
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Cleveland-Cliffs, Röhm, National Institute of Standards and Technology
Iron
Cleveland-Cliffs / AK Steel ARMCO Pure Iron Product Data Bulletin (07/2022): Table 1 typical physical properties, Table 2 typical mechanical properties after SRA/recrystallization anneal.
Plastic PMMA
Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)
  1. 1
    ARMCO Pure Iron Product Data Bulletin (2022)Cleveland-Cliffsarchived copyIron · Yield strength: typical (0.2% YS), hot rolled + SRA/recrystallization annealIron · Ultimate tensile strength: typical, SRA/recrystallization annealIron · Elongation at break: typical, gauge 4D0Iron · Young's modulus (stiffness): typical, after SRA/recrystallization annealIron · Density: typicalIron · Thermal conductivity: typical at 20 °CIron · Thermal expansion: mean, 20-399 °CIron · Specific heat: typicalIron · Melting point: typical
  2. 2
    PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
  3. 3
    Elastic Properties of Metals and Alloys, I. Iron, Nickel, and Iron-Nickel Alloys, J. Phys. Chem. Ref. Data 2 (1973)National Institute of Standards and Technologyarchived copyIron · Poisson's ratio: NIST critically evaluated best value (polycrystalline iron)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Iron stronger than Plastic PMMA?

Iron is stronger: its yield strength is 186 MPa against tensile strength 80 MPa for Plastic PMMA (2.33x).

Which is lighter, Iron or Plastic PMMA?

Plastic PMMA is lighter: 1,190 kg/m³ against 7,860 kg/m³ for Iron.

Which is stiffer, Iron or Plastic PMMA?

Iron is stiffer: Young's modulus 207 GPa against 3.3 GPa for Plastic PMMA, so the same part in Iron deflects less under the same load.

Which is lighter for the same job, Iron or Plastic PMMA?

For the same stiffness or strength: Iron is lighter for a stiff rod or tie (tension), stiff beam (bending); Plastic PMMA is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beIronPlastic PMMA
Stiff rod or tie (tension)lighter9.5x heavier
Stiff beam (bending)lighter20% heavier
Stiff panel or plate1.66x heavierlighter
Strong rod or tie2.84x heavierlighter
Strong beam3.76x heavierlighter
Strong panel or plate4.33x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Iron or Plastic PMMA?

Iron stretches further before it breaks: 38% elongation at break against 5.5% for Plastic PMMA.

Thermal

Which conducts heat better, Iron or Plastic PMMA?

Iron conducts heat better: 73.2 W/m·K against 0.19 W/m·K for Plastic PMMA.

Which expands less with temperature?

Iron expands less: 13.7 µm/m·K against 70 µm/m·K for Plastic PMMA.