Materials / Compare

Iron vs. Steel AISI 1045

Compare Iron vs. Steel AISI 1045 strength, stiffness, weight and thermal properties.

IronWrought
Steel AISI 1045Wrought
MechanicalIronSteel AISI 1045
Yield strength186MPa1producer-stated531MPa22.85x stronger
Ultimate tensile strength290MPa1producer-stated627MPa22.16x stronger
Elongation at break38%13.17x more ductilein 2 in12%2
Young's modulus (stiffness)207GPa1210GPa3
Density7,860kg/m³17,800kg/m³3
Strength to weight23.7kN·m/kg68.1kN·m/kg2.88x higher
Stiffness to weight26.3MN·m/kg26.9MN·m/kg2% higher
Poisson's ratio0.28240.33
Shear modulus80.7GPa80.8GPa
Bulk modulus158GPa175GPa11% higher
Speed of sound5,132m/s5,189m/s1% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronSteel AISI 1045
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronSteel AISI 1045
Strength against densityHigher and further left: stronger for its weight
ThermalIronSteel AISI 1045
Thermal conductivity73.2W/m·K140–45W/m·K3
Thermal expansionmean13.7µm/m·K112µm/m·K314% less
100 mm part over a 50 °C swing68.5µm growth60µm growth14% less
Specific heat450J/kg·K1460–480J/kg·K3
Heats up and cools (diffusivity)20.7mm²/s1.79x faster11.6mm²/s
Thermal shock resistance3,447W/m6,269W/m1.82x more resistant
Melting point1,532°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronSteel AISI 1045
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronSteel AISI 1045
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Cleveland-Cliffs, Niagara LaSalle, Ovako, National Institute of Standards and Technology
Iron
Cleveland-Cliffs / AK Steel ARMCO Pure Iron Product Data Bulletin (07/2022): Table 1 typical physical properties, Table 2 typical mechanical properties after SRA/recrystallization anneal.
Steel AISI 1045
AISI 1045 cold drawn bar (Niagara LaSalle) for mechanical; Ovako C45 (lists 'SAE 1045' as a similar designation) for physical constants
  1. 1
    ARMCO Pure Iron Product Data Bulletin (2022)Cleveland-Cliffsarchived copyIron · Yield strength: typical (0.2% YS), hot rolled + SRA/recrystallization annealIron · Ultimate tensile strength: typical, SRA/recrystallization annealIron · Elongation at break: typical, gauge 4D0Iron · Young's modulus (stiffness): typical, after SRA/recrystallization annealIron · Density: typicalIron · Thermal conductivity: typical at 20 °CIron · Thermal expansion: mean, 20-399 °CIron · Specific heat: typicalIron · Melting point: typical
  2. 2
    1045 PropertiesNiagara LaSallearchived copySteel AISI 1045 · Yield strength: producer-stated, cold drawnSteel AISI 1045 · Ultimate tensile strength: producer-stated, cold drawnSteel AISI 1045 · Elongation at break: in 2 in (50.8 mm)
  3. 3
    C45 Steel GradeOvakoSteel AISI 1045 · Young's modulus (stiffness): typicalSteel AISI 1045 · Density: typicalSteel AISI 1045 · Poisson's ratio: typicalSteel AISI 1045 · Thermal conductivity: typical range, ambientSteel AISI 1045 · Thermal expansion: typical, mean 20-300 °CSteel AISI 1045 · Specific heat: typical range, 50/100 °C
  4. 4
    Elastic Properties of Metals and Alloys, I. Iron, Nickel, and Iron-Nickel Alloys, J. Phys. Chem. Ref. Data 2 (1973)National Institute of Standards and Technologyarchived copyIron · Poisson's ratio: NIST critically evaluated best value (polycrystalline iron)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Iron stronger than Steel AISI 1045?

Steel AISI 1045 is stronger: its yield strength is 531 MPa against 186 MPa for Iron (2.85x).

Which is lighter, Iron or Steel AISI 1045?

Steel AISI 1045 is lighter: 7,800 kg/m³ against 7,860 kg/m³ for Iron.

Which is stiffer, Iron or Steel AISI 1045?

Steel AISI 1045 is stiffer: Young's modulus 210 GPa against 207 GPa for Iron, so the same part in Steel AISI 1045 deflects less under the same load.

Which is lighter for the same job, Iron or Steel AISI 1045?

For the same stiffness or strength: Steel AISI 1045 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beIronSteel AISI 1045
Stiff rod or tie (tension)2% heavierlighter
Stiff beam (bending)1% heavierlighter
Stiff panel or plate1% heavierlighter
Strong rod or tie2.88x heavierlighter
Strong beam2.03x heavierlighter
Strong panel or plate1.7x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Iron or Steel AISI 1045?

Iron stretches further before it breaks: 38% elongation at break against 12% for Steel AISI 1045.

Thermal

Which conducts heat better, Iron or Steel AISI 1045?

Iron conducts heat better: 73.2 W/m·K against 42.5 W/m·K for Steel AISI 1045.

Which expands less with temperature?

Steel AISI 1045 expands less: 12 µm/m·K against 13.7 µm/m·K for Iron.