Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values
1
Elektron AZ31B Sheet, Plate & Coil (Datasheet 482)Magnesium Elektronarchived copyMagnesium AZ31B-H24 · Yield strength: typical, H24, 0.5-6 mm, 0.2 % proof stressMagnesium AZ31B-H24 · Ultimate tensile strength: typical, H24, 0.5-6 mmMagnesium AZ31B-H24 · Elongation at break: typical, H24, 0.5-6 mm, gauge 5.65√AMagnesium AZ31B-H24 · Thermal conductivity: typical (temper/temperature not stated)Magnesium AZ31B-H24 · Thermal expansion: typical (temperature range not stated)Magnesium AZ31B-H24 · Specific heat: typical
2
Moplen HP501H Product DataLyondellBasellPlastic Polypropylene · Yield strength: typical, tensile stress at yield ISO 527Plastic Polypropylene · Young's modulus (stiffness): typical, tensile modulus ISO 527Plastic Polypropylene · Density: typical, 23 °C ISO 1183-1Plastic Polypropylene · Max service temperature: HDT 0.45 MPa (ISO 75B), unannealed
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseMagnesium AZ31B-H24 · Young's modulus (stiffness): typical (handbook physical constant)Magnesium AZ31B-H24 · Density: nominalMagnesium AZ31B-H24 · Poisson's ratio: typical (handbook physical constant)Magnesium AZ31B-H24 · Max service temperature: stated application limit
4
Typical Engineering Properties of PolypropyleneINEOS Olefins & Polymers USAarchived copyPlastic Polypropylene · Poisson's ratio: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)Plastic Polypropylene · Thermal conductivity: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)Plastic Polypropylene · Thermal expansion: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Magnesium AZ31B-H24 stronger than Plastic Polypropylene?
Magnesium AZ31B-H24 is stronger: its yield strength is 220 MPa against 33 MPa for Plastic Polypropylene (6.67x).
Which is lighter, Magnesium AZ31B-H24 or Plastic Polypropylene?
Plastic Polypropylene is lighter: 900 kg/m³ against 1,769 kg/m³ for Magnesium AZ31B-H24.
Which is stiffer, Magnesium AZ31B-H24 or Plastic Polypropylene?
Magnesium AZ31B-H24 is stiffer: Young's modulus 44.8 GPa against 1.45 GPa for Plastic Polypropylene, so the same part in Magnesium AZ31B-H24 deflects less under the same load.
Which is lighter for the same job, Magnesium AZ31B-H24 or Plastic Polypropylene?
For the same stiffness or strength: Magnesium AZ31B-H24 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Magnesium AZ31B-H24
Plastic Polypropylene
Stiff rod or tie (tension)
lighter
15.7x heavier
Stiff beam (bending)
lighter
2.83x heavier
Stiff panel or plate
lighter
1.6x heavier
Strong rod or tie
lighter
3.39x heavier
Strong beam
lighter
1.8x heavier
Strong panel or plate
lighter
31% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Magnesium AZ31B-H24 or Plastic Polypropylene?
Magnesium AZ31B-H24 conducts heat better: 76.9 W/m·K against 0.195 W/m·K for Plastic Polypropylene.
Which expands less with temperature?
Magnesium AZ31B-H24 expands less: 26.8 µm/m·K against 90 µm/m·K for Plastic Polypropylene.