Materials / Compare

PCB Board FR-4, 2 copper planes vs. Steel AISI 4340

Compare PCB Board FR-4, 2 copper planes vs. Steel AISI 4340 strength, stiffness, weight and thermal properties.

Change either side
PCB Board FR-4, 2 copper planesComposite
Steel AISI 4340Wrought
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)1,035MPasourcetypical, transverse
Ultimate tensile strength246–385MPasourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction (ASTM D3039)1,140MPasourcetypical, transverse
Elongation at breaknot sourced18%sourcetypical, transverse
Young's modulus (stiffness)21.9–25.8GPasourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction (ASTM D790-15e2); the copper planes are left out200GPasourceMIL-HDBK-5J design value (AISI 4340, quenched and tempered)
Densitynot sourced7,840kg/m³sourcetypical
Strength to weightnot sourced132kN·m/kg
Stiffness to weightnot sourced25.5MN·m/kg
Poisson's ratio0.171–0.177sourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction0.32sourceMIL-HDBK-5J design value (AISI 4340, quenched and tempered)
Shear modulus10.2GPa75.7GPa7.45x stiffer in shear
Bulk modulus12.2GPa185GPa
Speed of soundnot sourced5,049m/s
Thermal
Thermal conductivitynot sourced37.5W/m·Ksourcetypical
Thermal expansion13–14µm/m·Ksourcethe bare laminate's (fr4-370hr), in-plane X/Y-axis, below Tg (IPC-TM-650 2.4.24C)11.3µm/m·Ksourcemean, -18 to 93 °C
100 mm part over a 50 °C swing67.5µm growth56.5µm growth19% less
Specific heatnot sourced448J/kg·Ksourcetypical
Heats up and cools (diffusivity)not sourced10.7mm²/s
Thermal shock resistancenot sourced11,678W/m
Values forA whole circuit board read as one orthotropic plate: the JEDEC high-K thermal test board (JESD51-7, "2s2p"), 0.062 in (1.575 mm) thick with two internal solid copper planes 0.0014 in (1 oz) thick, as Texas Instruments SZZA017A Table 1 gives it. Copper C110 and the Isola 370HR laminate from this library; the layers conduct in parallel along the board and in series through it (boardStackup.ts). Its two 0.0028 in trace layers cover little of the board and are left out; vias are ignored. Mechanical values are the bare laminate's.Carpenter (Latrobe) Lescalloy 4340 VAC-ARC datasheet; mechanical row for 1100 °F temper; physical properties grade-level

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is PCB Board FR-4, 2 copper planes stronger than Steel AISI 4340?

Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against tensile strength 315 MPa for PCB Board FR-4, 2 copper planes (3.28x).

Which is stiffer, PCB Board FR-4, 2 copper planes or Steel AISI 4340?

Steel AISI 4340 is stiffer: Young's modulus 200 GPa against 23.9 GPa for PCB Board FR-4, 2 copper planes, so the same part in Steel AISI 4340 deflects less under the same load.

Which expands less with temperature?

Steel AISI 4340 expands less: 11.3 µm/m·K against 13.5 µm/m·K for PCB Board FR-4, 2 copper planes.

Among 73 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Steel AISI 4340
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Steel AISI 4340
Strength against density