Materials / PCB Board
PCB Board FR-4, 2 copper planes
PCB Board FR-4, 2 copper planes (JEDEC high-K 2s2p) strength, stiffness, density and thermal properties, with their source.
A panel in PCB Board FR-4, 2 copper planes, woven, clear-coated finish.
| Process | Composite |
|---|---|
| Mechanical | |
| Yield strength | not given (tensile used) |
| Ultimate tensile strength | 246–385MPasourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction (ASTM D3039) |
| Elongation at break | not sourced |
| Young's modulus (stiffness) | 21.9–25.8GPasourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction (ASTM D790-15e2); the copper planes are left out |
| Density | not sourced |
| Strength to weight | not sourced |
| Stiffness to weight | not sourced |
| Poisson's ratio | 0.171–0.177sourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction |
| Shear modulus | 10.2GPa |
| Bulk modulus | 12.2GPa |
| Speed of sound | not sourced |
| Thermal | |
| Thermal conductivity | not sourced |
| Thermal expansion | 13–14µm/m·Ksourcethe bare laminate's (fr4-370hr), in-plane X/Y-axis, below Tg (IPC-TM-650 2.4.24C) |
| 100 mm part over a 50 °C swing | 67.5µm growth |
| Specific heat | not sourced |
| Heats up and cools (diffusivity) | not sourced |
| Thermal shock resistance | not sourced |
| Values for | A whole circuit board read as one orthotropic plate: the JEDEC high-K thermal test board (JESD51-7, "2s2p"), 0.062 in (1.575 mm) thick with two internal solid copper planes 0.0014 in (1 oz) thick, as Texas Instruments SZZA017A Table 1 gives it. Copper C110 and the Isola 370HR laminate from this library; the layers conduct in parallel along the board and in series through it (boardStackup.ts). Its two 0.0028 in trace layers cover little of the board and are left out; vias are ignored. Mechanical values are the bare laminate's. |
Among 73 materials
Compare PCB Board FR-4, 2 copper planes with
Closest alternatives
- PCB Board FR-4, 2 copper planes vs. PCB Laminate FR-4
- PCB Board FR-4, 2 copper planes vs. Plastic PPS GF40
- PCB Board FR-4, 2 copper planes vs. Magnesium AZ31B-H24
- PCB Board FR-4, 2 copper planes vs. Magnesium AZ91D
- PCB Board FR-4, 2 copper planes vs. Aluminum
- PCB Board FR-4, 2 copper planes vs. Aluminum 6061-T6
- PCB Board FR-4, 2 copper planes vs. DMLS AlSi10Mg Aluminum
- PCB Board FR-4, 2 copper planes vs. Aluminum 2024-T351