Materials / Compare

PCB Laminate FR-4 vs. Plastic Nylon PA66

Compare PCB Laminate FR-4 vs. Plastic Nylon PA66 strength, stiffness, weight and thermal properties.

Change either side
PCB Laminate FR-4Composite
Plastic Nylon PA66Bulk polymer (molded or machined)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)85MPasourcetypical, dry
Ultimate tensile strength246–385MPasourcetypical, in-plane: cross direction .. length direction (ASTM D3039)not sourced
Flexural strength531–621MPasourcetypical: cross direction .. length direction (IPC-TM-650 2.4.4B)not sourced
Elongation at breaknot sourced30%sourcenominal strain at break, dry
Young's modulus (stiffness)21.9–25.8GPasourcetypical, in-plane: cross direction .. length direction (ASTM D790-15e2)3GPasourcetypical, dry
Density1,920kg/m³sourcetypical, 50% resin content; another FR-4 producer: Park Nelco N4000-6 (high-Tg multifunctional epoxy), not Isola 370HR1,130kg/m³sourcetypical
Strength to weight164kN·m/kg2.18x higher75.2kN·m/kg
Stiffness to weight12.4MN·m/kg4.68x higher2.65MN·m/kg
Poisson's ratio0.171–0.177sourcetypical, in-plane: cross direction .. length direction0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Shear modulus10.2GPa9.48x stiffer in shear1.07GPa
Bulk modulus12.2GPa5GPa
Speed of sound3,525m/s1,629m/s
Thermal
Thermal conductivity0.4W/m·Ksourcetypical (ASTM E1952); direction not stated by the sheet0.33W/m·Ksourcetypical
Thermal expansion13–14µm/m·Ksourcetypical, in-plane X/Y-axis, below Tg (IPC-TM-650 2.4.24C)98µm/m·Ksourcelongitudinal, 23-55 °C
100 mm part over a 50 °C swing67.5µm growth7.26x less490µm growth
Specific heat1,200–1,400J/kg·Ksourcetypical (ASTM E1461); another FR-4 producer: Park Nelco N4000-6 (high-Tg multifunctional epoxy), not Isola 370HR1,700J/kg·Ksourcetypical
Heats up and cools (diffusivity)0.16mm²/s0.172mm²/s7% faster
Thermal shock resistance324W/m5.65x more resistant57.2W/m
Melting pointnot sourced260°CsourceDSC
Glass transition180°Csourcetypical, DSC (IPC-TM-650 2.4.25C)not sourced
Max service temperature130°CsourceUL Relative Thermal Index (UL 796)101°CsourceIEC 60216 temperature index, 20000 h
Values forIsola 370HR FR-4 laminate (Polyclad PCL-FR-370HR, 180 C Tg multifunctional epoxy, E-glass fabric), copper removed; Isola data sheet Revision C, last updated April 15, 2021. Woven-glass laminate: the sheet gives in-plane values per weave direction (length / cross) and the Z-axis CTE separately; the solver is isotropic per material.BASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is PCB Laminate FR-4 stronger than Plastic Nylon PA66?

PCB Laminate FR-4 is stronger: its tensile strength is 315 MPa against yield strength 85 MPa for Plastic Nylon PA66 (3.71x).

Which is lighter, PCB Laminate FR-4 or Plastic Nylon PA66?

Plastic Nylon PA66 is lighter: 1,130 kg/m³ against 1,920 kg/m³ for PCB Laminate FR-4.

Which is stiffer, PCB Laminate FR-4 or Plastic Nylon PA66?

PCB Laminate FR-4 is stiffer: Young's modulus 23.9 GPa against 3 GPa for Plastic Nylon PA66, so the same part in PCB Laminate FR-4 deflects less under the same load.

Which is lighter for the same job, PCB Laminate FR-4 or Plastic Nylon PA66?

For the same stiffness or strength: PCB Laminate FR-4 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePCB Laminate FR-4Plastic Nylon PA66
Stiff rod or tie (tension)lighter4.68x heavier
Stiff beam (bending)lighter1.66x heavier
Stiff panel or platelighter17% heavier
Strong rod or tielighter2.18x heavier
Strong beamlighter41% heavier
Strong panel or platelighter13% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, PCB Laminate FR-4 or Plastic Nylon PA66?

PCB Laminate FR-4 conducts heat better: 0.4 W/m·K against 0.33 W/m·K for Plastic Nylon PA66.

Which expands less with temperature?

PCB Laminate FR-4 expands less: 13.5 µm/m·K against 98 µm/m·K for Plastic Nylon PA66.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelSiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30PCB Laminate FR-4Plastic Nylon PA66
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickSiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30PCB Laminate FR-4Plastic Nylon PA66
Strength against density