Materials / Compare

PCB Laminate FR-4 vs. Titanium Ti-6Al-4V

Compare PCB Laminate FR-4 vs. Titanium Ti-6Al-4V strength, stiffness, weight and thermal properties.

PCB Laminate FR-4Composite
Titanium Ti-6Al-4VWrought
MechanicalPCB Laminate FR-4Titanium Ti-6Al-4V
Yield strengthnot given (tensile used)885MPa1
Ultimate tensile strength246–385MPa2940MPa1
Flexural strength531–621MPa2not sourced
Elongation at breaknot sourced16%1
Young's modulus (stiffness)21.9–25.8GPa2107–122GPa3
Density1,920kg/m³42.31x lighter4,430kg/m³1
Strength to weight164kN·m/kg200kN·m/kg22% higher
Stiffness to weight12.4MN·m/kg25.8MN·m/kg2.08x higher
Poisson's ratio0.171–0.17720.3421
Shear modulus10.2GPa42.7GPa4.2x stiffer in shear
Bulk modulus12.2GPa121GPa9.9x higher
Speed of sound3,525m/s5,084m/s44% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Brass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteSiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30PCB Laminate FR-4Titanium Ti-6Al-4V
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Brass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickSiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30PCB Laminate FR-4Titanium Ti-6Al-4V
Strength against densityHigher and further left: stronger for its weight
ThermalPCB Laminate FR-4Titanium Ti-6Al-4V
Thermal conductivity0.4W/m·K26.6W/m·K316.5x more heat through a fin
Thermal expansion13–14µm/m·K29µm/m·K3
100 mm part over a 50 °C swing67.5µm growth45µm growth1.5x less
Specific heat1,200–1,400J/kg·K4580J/kg·K3
Heats up and cools (diffusivity)0.16mm²/s2.57mm²/s16x faster
Thermal shock resistance324W/m3,730W/m11.5x more resistant
Melting pointnot sourcedmelting range1,630–1,650°C1
Glass transition180°C2not sourced
Max service temperature130°C2400°C1
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Brass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickSiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30PCB Laminate FR-4Titanium Ti-6Al-4V
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Brass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodSiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30PCB Laminate FR-4Titanium Ti-6Al-4V
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: TIMET, Isola, Park Electrochemical (Nelco)
PCB Laminate FR-4
Isola 370HR FR-4 laminate (Polyclad PCL-FR-370HR, 180 C Tg multifunctional epoxy, E-glass fabric), copper removed; Isola data sheet Revision C, last updated April 15, 2021. Woven-glass laminate: the sheet gives in-plane values per weave direction (length / cross) and the Z-axis CTE separately; the solver is isotropic per material.
Titanium Ti-6Al-4V
TIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties
  1. 1
    TIMETAL 6-4 PropertiesTIMETarchived copyTitanium Ti-6Al-4V · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium Ti-6Al-4V · Ultimate tensile strength: typical, plate, annealedTitanium Ti-6Al-4V · Elongation at break: typical, in 2 in., plate annealedTitanium Ti-6Al-4V · Density: nominalTitanium Ti-6Al-4V · Poisson's ratio: mean of TIMET measurementsTitanium Ti-6Al-4V · Melting point: melting rangeTitanium Ti-6Al-4V · Max service temperature: upper recommended use temperature
  2. 2
    370HR Laminate and Prepreg Data SheetIsolaarchived copyPCB Laminate FR-4 · Ultimate tensile strength: typical, in-plane: cross direction .. length direction (ASTM D3039)PCB Laminate FR-4 · Flexural strength: typical: cross direction .. length direction (IPC-TM-650 2.4.4B)PCB Laminate FR-4 · Young's modulus (stiffness): typical, in-plane: cross direction .. length direction (ASTM D790-15e2)PCB Laminate FR-4 · Poisson's ratio: typical, in-plane: cross direction .. length directionPCB Laminate FR-4 · Thermal conductivity: typical (ASTM E1952); direction not stated by the sheetPCB Laminate FR-4 · Thermal expansion: typical, in-plane X/Y-axis, below Tg (IPC-TM-650 2.4.24C)PCB Laminate FR-4 · Glass transition: typical, DSC (IPC-TM-650 2.4.25C)PCB Laminate FR-4 · Max service temperature: UL Relative Thermal Index (UL 796)
  3. 3
    TIMETAL 6-4 Data SheetTIMETarchived copyTitanium Ti-6Al-4V · Young's modulus (stiffness): typical range, 20 °CTitanium Ti-6Al-4V · Thermal conductivity: typical, 20 °C, mill annealedTitanium Ti-6Al-4V · Thermal expansion: typical, mean 0-100 °CTitanium Ti-6Al-4V · Specific heat: typical, 20 °C
  4. 4
    N4000-6 Laminate Data Sheet (2006)Park Electrochemical (Nelco)archived copyPCB Laminate FR-4 · Density: typical, 50% resin content; another FR-4 producer: Park Nelco N4000-6 (high-Tg multifunctional epoxy), not Isola 370HRPCB Laminate FR-4 · Specific heat: typical (ASTM E1461); another FR-4 producer: Park Nelco N4000-6 (high-Tg multifunctional epoxy), not Isola 370HR

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is PCB Laminate FR-4 stronger than Titanium Ti-6Al-4V?

Titanium Ti-6Al-4V is stronger: its yield strength is 885 MPa against tensile strength 315 MPa for PCB Laminate FR-4 (2.81x).

Which is lighter, PCB Laminate FR-4 or Titanium Ti-6Al-4V?

PCB Laminate FR-4 is lighter: 1,920 kg/m³ against 4,430 kg/m³ for Titanium Ti-6Al-4V.

Which is stiffer, PCB Laminate FR-4 or Titanium Ti-6Al-4V?

Titanium Ti-6Al-4V is stiffer: Young's modulus 115 GPa against 23.9 GPa for PCB Laminate FR-4, so the same part in Titanium Ti-6Al-4V deflects less under the same load.

Which is lighter for the same job, PCB Laminate FR-4 or Titanium Ti-6Al-4V?

For the same stiffness or strength: PCB Laminate FR-4 is lighter for a stiff beam (bending), stiff panel or plate, strong beam, strong panel or plate; Titanium Ti-6Al-4V is lighter for a stiff rod or tie (tension), strong rod or tie.

Part that must bePCB Laminate FR-4Titanium Ti-6Al-4V
Stiff rod or tie (tension)2.08x heavierlighter
Stiff beam (bending)lighter5% heavier
Stiff panel or platelighter37% heavier
Strong rod or tie22% heavierlighter
Strong beamlighter16% heavier
Strong panel or platelighter38% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, PCB Laminate FR-4 or Titanium Ti-6Al-4V?

Titanium Ti-6Al-4V conducts heat better: 6.6 W/m·K against 0.4 W/m·K for PCB Laminate FR-4.

Which expands less with temperature?

Titanium Ti-6Al-4V expands less: 9 µm/m·K against 13.5 µm/m·K for PCB Laminate FR-4.

Related comparisons