Materials / Compare

Plastic ABS vs. Stainless Steel 303

Compare Plastic ABS vs. Stainless Steel 303 strength, stiffness, weight and thermal properties.

Plastic ABS3D printed (FDM)
Stainless Steel 303Wrought
MechanicalPlastic ABSStainless Steel 303
Yield strength38.1MPa1Outokumpu typical275MPa27.22x stronger
Ultimate tensile strength38.1MPa1Outokumpu typical585MPa215.4x stronger
Flexural strength61.1MPa1not sourced
Elongation at break4.6%1Outokumpu typical35%27.61x more ductile
Young's modulus (stiffness)1.96GPa1at RT200GPa2102x stiffer
Density1,100kg/m³17.18x lighterat RT7,900kg/m³2
Strength to weight34.6kN·m/kg34.8kN·m/kg
Stiffness to weight1.78MN·m/kg25.3MN·m/kg14.2x higher
Poisson's ratiobase material0.393design value0.34
Shear modulus0.706GPa76.9GPa109x stiffer in shear
Bulk modulus2.97GPa167GPa56.1x higher
Speed of sound1,336m/s5,032m/s3.77x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABSStainless Steel 303
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABSStainless Steel 303
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic ABSStainless Steel 303
Thermal conductivitybase material0.17W/m·K5at RT15W/m·K288.2x more heat through a fin
Thermal expansionbase material80–110µm/m·K5mean16µm/m·K2
100 mm part over a 50 °C swing475µm growth80µm growth5.94x less
Specific heatnot sourcedat RT500J/kg·K2
Heats up and cools (diffusivity)not sourced3.8mm²/s
Thermal shock resistance21.2W/m902W/m42.6x more resistant
Glass transition101°C1not sourced
Max service temperatureHDT 0.455 MPa86.6°C1continuous871°C6
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABSStainless Steel 303
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABSStainless Steel 303
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources6 documents: UltiMaker, Outokumpu, Covestro, Steel Construction Institute, INEOS Styrolution, Carpenter Technology
Plastic ABS
Ultimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.
Stainless Steel 303
1.4305 / UNS S30300, Outokumpu typical values (hot rolled, solution annealed) from 'Steel Grades, Properties and Global Standards'; max service from Carpenter CarTech 303 datasheet
  1. 1
    Ultimaker ABS Technical Data Sheet, v5.00UltiMakerarchived copyPlastic ABS · Yield strength: typicalPlastic ABS · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic ABS · Flexural strength: typicalPlastic ABS · Elongation at break: typicalPlastic ABS · Young's modulus (stiffness): typicalPlastic ABS · Density: typicalPlastic ABS · Glass transition: typicalPlastic ABS · Max service temperature: HDT 0.455 MPa (printed specimens)
  2. 2
    Steel Grades, Properties and Global StandardsOutokumpuarchived copyStainless Steel 303 · Yield strength: Outokumpu typical (product P = hot rolled plate, transverse)Stainless Steel 303 · Ultimate tensile strength: Outokumpu typicalStainless Steel 303 · Elongation at break: Outokumpu typical, A5Stainless Steel 303 · Young's modulus (stiffness): at RT (Table 12)Stainless Steel 303 · Density: at RTStainless Steel 303 · Thermal conductivity: at RTStainless Steel 303 · Thermal expansion: mean, 20–100 °CStainless Steel 303 · Specific heat: at RT
  3. 3
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic ABS · Poisson's ratio: base material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)
  4. 4
    Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 303 · Poisson's ratio: design value (structural stainless steels)
  5. 5
    Terluran GP-22 (ABS) Product Data SheetINEOS StyrolutionPlastic ABS · Thermal conductivity: base material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typicalPlastic ABS · Thermal expansion: base material: INEOS Styrolution Terluran GP-22 injection-molding ABS, range
  6. 6
    Carpenter Stainless Type 303 Data SheetCarpenter Technologyarchived copyStainless Steel 303 · Max service temperature: continuous, scaling limit

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Plastic ABS stronger than Stainless Steel 303?

Stainless Steel 303 is stronger: its yield strength is 275 MPa against 38.1 MPa for Plastic ABS (7.22x).

Which is lighter, Plastic ABS or Stainless Steel 303?

Plastic ABS is lighter: 1,100 kg/m³ against 7,900 kg/m³ for Stainless Steel 303.

Which is stiffer, Plastic ABS or Stainless Steel 303?

Stainless Steel 303 is stiffer: Young's modulus 200 GPa against 1.96 GPa for Plastic ABS, so the same part in Stainless Steel 303 deflects less under the same load.

Which is lighter for the same job, Plastic ABS or Stainless Steel 303?

For the same stiffness or strength: Plastic ABS is lighter for a stiff panel or plate, strong beam, strong panel or plate; Stainless Steel 303 is lighter for a stiff rod or tie (tension), stiff beam (bending).

Part that must bePlastic ABSStainless Steel 303
Stiff rod or tie (tension)14.2x heavierlighter
Stiff beam (bending)41% heavierlighter
Stiff panel or platelighter1.54x heavier
Strong rod or tieabout equalabout equal
Strong beamlighter1.92x heavier
Strong panel or platelighter2.67x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic ABS or Stainless Steel 303?

Stainless Steel 303 stretches further before it breaks: 35% elongation at break against 4.6% for Plastic ABS.

Thermal

Which conducts heat better, Plastic ABS or Stainless Steel 303?

Stainless Steel 303 conducts heat better: 15 W/m·K against 0.17 W/m·K for Plastic ABS.

Which expands less with temperature?

Stainless Steel 303 expands less: 16 µm/m·K against 95 µm/m·K for Plastic ABS.

Related comparisons