Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)
4
Typical Engineering Properties of High Density PolyethyleneINEOS Olefins & Polymers USAarchived copyPlastic HDPE · Poisson's ratio: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal conductivity: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal expansion: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Specific heat: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic HDPE stronger than Steel AISI 4340?
Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against 24 MPa for Plastic HDPE (43.1x).
Which is lighter, Plastic HDPE or Steel AISI 4340?
Plastic HDPE is lighter: 950 kg/m³ against 7,840 kg/m³ for Steel AISI 4340.
Which is stiffer, Plastic HDPE or Steel AISI 4340?
Steel AISI 4340 is stiffer: Young's modulus 200 GPa against 0.9 GPa for Plastic HDPE, so the same part in Steel AISI 4340 deflects less under the same load.
Which is lighter for the same job, Plastic HDPE or Steel AISI 4340?
For the same stiffness or strength: Plastic HDPE is lighter for a stiff panel or plate, strong panel or plate; Steel AISI 4340 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam.
Part that must be
Plastic HDPE
Steel AISI 4340
Stiff rod or tie (tension)
26.9x heavier
lighter
Stiff beam (bending)
1.81x heavier
lighter
Stiff panel or plate
lighter
36% heavier
Strong rod or tie
5.23x heavier
lighter
Strong beam
49% heavier
lighter
Strong panel or plate
lighter
26% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Plastic HDPE or Steel AISI 4340?
Steel AISI 4340 conducts heat better: 37.5 W/m·K against 0.445 W/m·K for Plastic HDPE.
Which expands less with temperature?
Steel AISI 4340 expands less: 11.3 µm/m·K against 120 µm/m·K for Plastic HDPE.