Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Hostalen 23050 B Product DataLyondellBasellPlastic HDPE · Yield strength: typical, tensile stress at yield 23 °C, 50 mm/min ISO 527Plastic HDPE · Young's modulus (stiffness): typical, tensile modulus 23 °C ISO 527Plastic HDPE · Density: typical, ISO 1183
2
TIMETAL 6-4 PropertiesTIMETarchived copyTitanium · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium · Ultimate tensile strength: typical, plate, annealedTitanium · Elongation at break: typical, in 2 in., plate annealedTitanium · Density: nominalTitanium · Poisson's ratio: mean of TIMET measurementsTitanium · Melting point: melting rangeTitanium · Max service temperature: upper recommended use temperature
3
TIMETAL 6-4 Data SheetTIMETarchived copyTitanium · Young's modulus (stiffness): typical range, 20 °CTitanium · Thermal conductivity: typical, 20 °C, mill annealedTitanium · Thermal expansion: typical, mean 0-100 °CTitanium · Specific heat: typical, 20 °C
4
Typical Engineering Properties of High Density PolyethyleneINEOS Olefins & Polymers USAarchived copyPlastic HDPE · Poisson's ratio: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal conductivity: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal expansion: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Specific heat: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic HDPE stronger than Titanium?
Titanium is stronger: its yield strength is 885 MPa against 24 MPa for Plastic HDPE (36.9x).
Which is lighter, Plastic HDPE or Titanium?
Plastic HDPE is lighter: 950 kg/m³ against 4,430 kg/m³ for Titanium.
Which is stiffer, Plastic HDPE or Titanium?
Titanium is stiffer: Young's modulus 115 GPa against 0.9 GPa for Plastic HDPE, so the same part in Titanium deflects less under the same load.
Which is lighter for the same job, Plastic HDPE or Titanium?
For the same stiffness or strength: Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic HDPE
Titanium
Stiff rod or tie (tension)
27.3x heavier
lighter
Stiff beam (bending)
2.42x heavier
lighter
Stiff panel or plate
8% heavier
lighter
Strong rod or tie
7.91x heavier
lighter
Strong beam
2.38x heavier
lighter
Strong panel or plate
30% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Plastic HDPE or Titanium?
Titanium conducts heat better: 6.6 W/m·K against 0.445 W/m·K for Plastic HDPE.
Which expands less with temperature?
Titanium expands less: 9 µm/m·K against 120 µm/m·K for Plastic HDPE.