Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: American Institute of Steel Construction, Sumitomo Chemical, bauforumstahl (ArcelorMittal), Ovako
Plastic LCP GF30
Sumitomo Chemical SUMIKASUPER LCP E6006L (30% glass fibre; high strength, low shrinkage); SUMIKASUPER LCP Technical Note, Version 04 / Nov. 2023, typical values.
Steel A992
ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
1
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel A992 · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel A992 · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel A992 · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
2
SUMIKASUPER LCP Technical Note, Version 04 (2023)Sumitomo Chemicalarchived copyPlastic LCP GF30 · Ultimate tensile strength: tensile strength (ISO 527)Plastic LCP GF30 · Flexural strength: typical (ISO 178)Plastic LCP GF30 · Elongation at break: tensile elongation (ISO 527)Plastic LCP GF30 · Young's modulus (stiffness): tensile modulus (ISO 527)Plastic LCP GF30 · Density: typicalPlastic LCP GF30 · Thermal conductivity: hot disk (ISO 22007-2), temperature not statedPlastic LCP GF30 · Thermal expansion: flow direction (MD), mean 50-150 °CPlastic LCP GF30 · Specific heat: ASTM E1269, temperature not statedPlastic LCP GF30 · Max service temperature: HDT 1.8 MPa (ISO 75)
3
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel A992 · Young's modulus (stiffness): design value (AISC 360-16)Steel A992 · Poisson's ratio: design value (AISC 360-16 Commentary)
4
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel A992 · Density: nominal (constructional data)Steel A992 · Thermal conductivity: nominal at 20 °CSteel A992 · Thermal expansion: nominal (constructional data, no temperature range stated)
5
S275JR Steel GradeOvakoSteel A992 · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic LCP GF30 stronger than Steel A992?
Steel A992 is stronger: its yield strength is 385 MPa against tensile strength 115 MPa for Plastic LCP GF30 (3.35x).
Which is lighter, Plastic LCP GF30 or Steel A992?
Plastic LCP GF30 is lighter: 1,610 kg/m³ against 7,850 kg/m³ for Steel A992.
Which is stiffer, Plastic LCP GF30 or Steel A992?
Steel A992 is stiffer: Young's modulus 200 GPa against 11.5 GPa for Plastic LCP GF30, so the same part in Steel A992 deflects less under the same load.
Which is lighter for the same job, Plastic LCP GF30 or Steel A992?
For the same stiffness or strength: Plastic LCP GF30 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Steel A992 is lighter for a stiff rod or tie (tension).
Part that must be
Plastic LCP GF30
Steel A992
Stiff rod or tie (tension)
3.57x heavier
lighter
Stiff beam (bending)
lighter
17% heavier
Stiff panel or plate
lighter
1.88x heavier
Strong rod or tie
lighter
46% heavier
Strong beam
lighter
2.18x heavier
Strong panel or plate
lighter
2.66x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic LCP GF30 or Steel A992?
Steel A992 stretches further before it breaks: 24.2% elongation at break against 1.5% for Plastic LCP GF30.
Thermal
Which conducts heat better, Plastic LCP GF30 or Steel A992?
Steel A992 conducts heat better: 48 W/m·K against 0.5 W/m·K for Plastic LCP GF30.
Which expands less with temperature?
Steel A992 expands less: 12 µm/m·K against 20 µm/m·K for Plastic LCP GF30.