Materials / Compare

Plastic Nylon PA6 vs. Plastic Polypropylene

Compare Plastic Nylon PA6 vs. Plastic Polypropylene strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon PA6Bulk polymer (molded or machined)
Plastic PolypropyleneBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength90MPasourcetypical, dry33MPasourcetypical, tensile stress at yield ISO 527
Ultimate tensile strengthnot sourcednot sourced
Elongation at break10%sourcenominal strain at break, drynot sourced
Young's modulus (stiffness)3.5GPasourcetypical, dry1.45GPasourcetypical, tensile modulus ISO 527
Density1,130kg/m³sourcetypical900kg/m³sourcetypical, 23 °C ISO 1183-1
Strength to weight79.6kN·m/kg2.17x higher36.7kN·m/kg
Stiffness to weight3.1MN·m/kg1.92x higher1.61MN·m/kg
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)0.42sourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
Shear modulus1.25GPa2.45x stiffer in shear0.511GPa
Bulk modulus5.83GPa3.02GPa
Speed of sound1,760m/s1,269m/s
Thermal
Thermal conductivity0.33W/m·Ksourcetypical0.17–0.22W/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
Thermal expansion102µm/m·Ksourcelongitudinal, 23-55 °C80–100µm/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
100 mm part over a 50 °C swing510µm growth450µm growth13% less
Specific heat1,700J/kg·Ksourcetypicalnot sourced
Heats up and cools (diffusivity)0.172mm²/snot sourced
Thermal shock resistance49.9W/m1.75x more resistant28.6W/m
Melting point220°CsourceDSCnot sourced
Max service temperature87°CsourceIEC 60216 temperature index, 20000 h90°CsourceHDT 0.45 MPa (ISO 75B), unannealed
Values forBASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic Nylon PA6 stronger than Plastic Polypropylene?

Plastic Nylon PA6 is stronger: its yield strength is 90 MPa against 33 MPa for Plastic Polypropylene (2.73x).

Which is lighter, Plastic Nylon PA6 or Plastic Polypropylene?

Plastic Polypropylene is lighter: 900 kg/m³ against 1,130 kg/m³ for Plastic Nylon PA6.

Which is stiffer, Plastic Nylon PA6 or Plastic Polypropylene?

Plastic Nylon PA6 is stiffer: Young's modulus 3.5 GPa against 1.45 GPa for Plastic Polypropylene, so the same part in Plastic Nylon PA6 deflects less under the same load.

Which is lighter for the same job, Plastic Nylon PA6 or Plastic Polypropylene?

For the same stiffness or strength: Plastic Nylon PA6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic Nylon PA6Plastic Polypropylene
Stiff rod or tie (tension)lighter1.92x heavier
Stiff beam (bending)lighter24% heavier
Stiff panel or platelighter7% heavier
Strong rod or tielighter2.17x heavier
Strong beamlighter1.55x heavier
Strong panel or platelighter32% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Nylon PA6 or Plastic Polypropylene?

Plastic Nylon PA6 conducts heat better: 0.33 W/m·K against 0.195 W/m·K for Plastic Polypropylene.

Which expands less with temperature?

Plastic Polypropylene expands less: 90 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon PA6Plastic Polypropylene
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon PA6Plastic Polypropylene
Strength against density

Related comparisons