Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
BASF Ultradur B 4300 G6 (PBT, 30% glass fibre), injection moulding grade; product information sheet 09/2026, typical values for uncoloured product at 23 °C.
TIMETAL 6-4 PropertiesTIMETarchived copyTitanium · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium · Ultimate tensile strength: typical, plate, annealedTitanium · Elongation at break: typical, in 2 in., plate annealedTitanium · Density: nominalTitanium · Poisson's ratio: mean of TIMET measurementsTitanium · Melting point: melting rangeTitanium · Max service temperature: upper recommended use temperature
2
Ultradur B 4300 G6 Product InformationBASFPlastic PBT GF30 · Ultimate tensile strength: stress at break, 23 °CPlastic PBT GF30 · Flexural strength: typical, 23 °CPlastic PBT GF30 · Elongation at break: strain at break, 23 °CPlastic PBT GF30 · Young's modulus (stiffness): typical, 23 °CPlastic PBT GF30 · Density: typicalPlastic PBT GF30 · Thermal conductivity: typical (DIN 52612-1)Plastic PBT GF30 · Thermal expansion: longitudinal (flow), mean 23-55 °CPlastic PBT GF30 · Specific heat: typical, 23 °CPlastic PBT GF30 · Melting point: DSC (ISO 11357)Plastic PBT GF30 · Max service temperature: HDT 1.8 MPa
3
TIMETAL 6-4 Data SheetTIMETarchived copyTitanium · Young's modulus (stiffness): typical range, 20 °CTitanium · Thermal conductivity: typical, 20 °C, mill annealedTitanium · Thermal expansion: typical, mean 0-100 °CTitanium · Specific heat: typical, 20 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic PBT GF30 stronger than Titanium?
Titanium is stronger: its yield strength is 885 MPa against tensile strength 140 MPa for Plastic PBT GF30 (6.32x).
Which is lighter, Plastic PBT GF30 or Titanium?
Plastic PBT GF30 is lighter: 1,530 kg/m³ against 4,430 kg/m³ for Titanium.
Which is stiffer, Plastic PBT GF30 or Titanium?
Titanium is stiffer: Young's modulus 115 GPa against 9.8 GPa for Plastic PBT GF30, so the same part in Titanium deflects less under the same load.
Which is lighter for the same job, Plastic PBT GF30 or Titanium?
For the same stiffness or strength: Plastic PBT GF30 is lighter for a stiff panel or plate, strong panel or plate; Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam.
Part that must be
Plastic PBT GF30
Titanium
Stiff rod or tie (tension)
4.04x heavier
lighter
Stiff beam (bending)
18% heavier
lighter
Stiff panel or plate
lighter
28% heavier
Strong rod or tie
2.18x heavier
lighter
Strong beam
18% heavier
lighter
Strong panel or plate
lighter
15% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PBT GF30 or Titanium?
Titanium stretches further before it breaks: 16% elongation at break against 3% for Plastic PBT GF30.
Thermal
Which conducts heat better, Plastic PBT GF30 or Titanium?
Titanium conducts heat better: 6.6 W/m·K against 0.27 W/m·K for Plastic PBT GF30.
Which expands less with temperature?
Titanium expands less: 9 µm/m·K against 25 µm/m·K for Plastic PBT GF30.