Materials / Compare

Plastic PLA vs. SLA Resin Tough 2000

Compare Plastic PLA vs. SLA Resin Tough 2000 strength, stiffness, weight and thermal properties.

Change either side
Plastic PLA3D printed (FDM)
SLA Resin Tough 20003D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength52.5MPasourcetypical30% stronger40.4MPasourcetypical
Ultimate tensile strength52.5MPasourcetypical, peak stress (= stress at yield)40.4MPasourcetypical
Flexural strength96.8MPasourcetypical44% stronger in bending67MPasourcetypical
Elongation at break7.8%sourcetypical79%sourcetypical10.1x more ductile
Young's modulus (stiffness)3.25GPasourcetypical1.81x stiffer1.8GPasourcetypical
Density1,240kg/m³sourcetypical1,090kg/m³sourcetypical14% lighter
Strength to weight42.3kN·m/kg14% higher37.1kN·m/kg
Stiffness to weight2.62MN·m/kg1.59x higher1.65MN·m/kg
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,619m/s1,285m/s
Thermal
Thermal conductivity0.13W/m·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °Cnot sourced
Thermal expansionnot sourced134µm/m·Ksourcemean 0-150 °C
100 mm part over a 50 °C swingnot sourced671µm growth
Specific heat1,200J/kg·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °Cnot sourced
Heats up and cools (diffusivity)0.0874mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Melting point152°Csourcetypicalnot sourced
Glass transition59.1°Csourcetypical112°CsourceDMA
Max service temperature58.8°CsourceHDT 0.455 MPa (printed specimens)57°CsourceHDT 1.8 MPa
Values forUltimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PLA and SLA Resin Tough 2000 are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic PLA stronger than SLA Resin Tough 2000?

Plastic PLA is stronger: its yield strength is 52.5 MPa against 40.4 MPa for SLA Resin Tough 2000 (30%).

Which is lighter, Plastic PLA or SLA Resin Tough 2000?

SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 1,240 kg/m³ for Plastic PLA.

Which is stiffer, Plastic PLA or SLA Resin Tough 2000?

Plastic PLA is stiffer: Young's modulus 3.25 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Plastic PLA deflects less under the same load.

Which is lighter for the same job, Plastic PLA or SLA Resin Tough 2000?

For the same stiffness or strength: Plastic PLA is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam.

Part that must bePlastic PLASLA Resin Tough 2000
Stiff rod or tie (tension)lighter1.59x heavier
Stiff beam (bending)lighter18% heavier
Stiff panel or platelighter7% heavier
Strong rod or tielighter14% heavier
Strong beamlighter5% heavier
Strong panel or plateabout equalabout equal

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic PLA or SLA Resin Tough 2000?

SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 7.8% for Plastic PLA.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PLASLA Resin Tough 2000
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PLASLA Resin Tough 2000
Strength against density