Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
TIMETAL 6-4 PropertiesTIMETarchived copyTitanium Ti-6Al-4V · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium Ti-6Al-4V · Ultimate tensile strength: typical, plate, annealedTitanium Ti-6Al-4V · Elongation at break: typical, in 2 in., plate annealedTitanium Ti-6Al-4V · Density: nominalTitanium Ti-6Al-4V · Poisson's ratio: mean of TIMET measurementsTitanium Ti-6Al-4V · Melting point: melting rangeTitanium Ti-6Al-4V · Max service temperature: upper recommended use temperature
3
TIMETAL 6-4 Data SheetTIMETarchived copyTitanium Ti-6Al-4V · Young's modulus (stiffness): typical range, 20 °CTitanium Ti-6Al-4V · Thermal conductivity: typical, 20 °C, mill annealedTitanium Ti-6Al-4V · Thermal expansion: typical, mean 0-100 °CTitanium Ti-6Al-4V · Specific heat: typical, 20 °C
4
Engineering Properties of Ingeo BiopolymerNatureWorksarchived copyPlastic PLA · Thermal conductivity: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °CPlastic PLA · Specific heat: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Plastic PLA is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Plastic PLA stronger than Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V is stronger: its yield strength is 885 MPa against 52.5 MPa for Plastic PLA (16.9x).
Which is lighter, Plastic PLA or Titanium Ti-6Al-4V?
Plastic PLA is lighter: 1,240 kg/m³ against 4,430 kg/m³ for Titanium Ti-6Al-4V.
Which is stiffer, Plastic PLA or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V is stiffer: Young's modulus 115 GPa against 3.25 GPa for Plastic PLA, so the same part in Titanium Ti-6Al-4V deflects less under the same load.
Which is lighter for the same job, Plastic PLA or Titanium Ti-6Al-4V?
For the same stiffness or strength: Plastic PLA is lighter for a stiff panel or plate; Titanium Ti-6Al-4V is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic PLA
Titanium Ti-6Al-4V
Stiff rod or tie (tension)
9.86x heavier
lighter
Stiff beam (bending)
1.66x heavier
lighter
Stiff panel or plate
lighter
9% heavier
Strong rod or tie
4.72x heavier
lighter
Strong beam
1.84x heavier
lighter
Strong panel or plate
15% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PLA or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V stretches further before it breaks: 16% elongation at break against 7.8% for Plastic PLA.
Thermal
Which conducts heat better, Plastic PLA or Titanium Ti-6Al-4V?
Titanium Ti-6Al-4V conducts heat better: 6.6 W/m·K against 0.13 W/m·K for Plastic PLA.