Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 1018 · Young's modulus (stiffness): base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Density: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Poisson's ratio: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Thermal conductivity: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Specific heat: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
4
S275JR Steel GradeOvakoSteel AISI 1018 · Thermal expansion: base material: unalloyed carbon steel, Ovako family table (S275JR, 'none alloyed structural steels', C <= 0.21%); mean 20-300 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic PMMA stronger than Steel AISI 1018?
Steel AISI 1018 is stronger: its yield strength is 372 MPa against tensile strength 80 MPa for Plastic PMMA (4.65x).
Which is lighter, Plastic PMMA or Steel AISI 1018?
Plastic PMMA is lighter: 1,190 kg/m³ against 7,861 kg/m³ for Steel AISI 1018.
Which is stiffer, Plastic PMMA or Steel AISI 1018?
Steel AISI 1018 is stiffer: Young's modulus 200 GPa against 3.3 GPa for Plastic PMMA, so the same part in Steel AISI 1018 deflects less under the same load.
Which is lighter for the same job, Plastic PMMA or Steel AISI 1018?
For the same stiffness or strength: Plastic PMMA is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Steel AISI 1018 is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
Plastic PMMA
Steel AISI 1018
Stiff rod or tie (tension)
9.17x heavier
lighter
Stiff beam (bending)
18% heavier
lighter
Stiff panel or plate
lighter
1.68x heavier
Strong rod or tie
lighter
42% heavier
Strong beam
lighter
2.37x heavier
Strong panel or plate
lighter
3.06x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PMMA or Steel AISI 1018?
Steel AISI 1018 stretches further before it breaks: 15% elongation at break against 5.5% for Plastic PMMA.
Thermal
Which conducts heat better, Plastic PMMA or Steel AISI 1018?
Steel AISI 1018 conducts heat better: 51.9 W/m·K against 0.19 W/m·K for Plastic PMMA.
Which expands less with temperature?
Steel AISI 1018 expands less: 12 µm/m·K against 70 µm/m·K for Plastic PMMA.