Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
TIMETAL 6-4 PropertiesTIMETarchived copyTitanium · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium · Ultimate tensile strength: typical, plate, annealedTitanium · Elongation at break: typical, in 2 in., plate annealedTitanium · Density: nominalTitanium · Poisson's ratio: mean of TIMET measurementsTitanium · Melting point: melting rangeTitanium · Max service temperature: upper recommended use temperature
2
PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
3
TIMETAL 6-4 Data SheetTIMETarchived copyTitanium · Young's modulus (stiffness): typical range, 20 °CTitanium · Thermal conductivity: typical, 20 °C, mill annealedTitanium · Thermal expansion: typical, mean 0-100 °CTitanium · Specific heat: typical, 20 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic PMMA stronger than Titanium?
Titanium is stronger: its yield strength is 885 MPa against tensile strength 80 MPa for Plastic PMMA (11.1x).
Which is lighter, Plastic PMMA or Titanium?
Plastic PMMA is lighter: 1,190 kg/m³ against 4,430 kg/m³ for Titanium.
Which is stiffer, Plastic PMMA or Titanium?
Titanium is stiffer: Young's modulus 115 GPa against 3.3 GPa for Plastic PMMA, so the same part in Titanium deflects less under the same load.
Which is lighter for the same job, Plastic PMMA or Titanium?
For the same stiffness or strength: Plastic PMMA is lighter for a stiff panel or plate, strong panel or plate; Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam.
Part that must be
Plastic PMMA
Titanium
Stiff rod or tie (tension)
9.32x heavier
lighter
Stiff beam (bending)
1.58x heavier
lighter
Stiff panel or plate
lighter
14% heavier
Strong rod or tie
2.97x heavier
lighter
Strong beam
33% heavier
lighter
Strong panel or plate
lighter
12% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PMMA or Titanium?
Titanium stretches further before it breaks: 16% elongation at break against 5.5% for Plastic PMMA.
Thermal
Which handles higher temperatures, Plastic PMMA or Titanium?
Titanium does: 400 °C against 80 °C for Plastic PMMA.
Which conducts heat better, Plastic PMMA or Titanium?
Titanium conducts heat better: 6.6 W/m·K against 0.19 W/m·K for Plastic PMMA.
Which expands less with temperature?
Titanium expands less: 9 µm/m·K against 70 µm/m·K for Plastic PMMA.