Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: LyondellBasell, Formlabs, INEOS Olefins & Polymers USA
Plastic Polypropylene
LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values
SLA Resin Elastic 50A
Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.
1
Moplen HP501H Product DataLyondellBasellPlastic Polypropylene · Yield strength: typical, tensile stress at yield ISO 527Plastic Polypropylene · Young's modulus (stiffness): typical, tensile modulus ISO 527Plastic Polypropylene · Density: typical, 23 °C ISO 1183-1Plastic Polypropylene · Max service temperature: HDT 0.45 MPa (ISO 75B), unannealed
Typical Engineering Properties of PolypropyleneINEOS Olefins & Polymers USAarchived copyPlastic Polypropylene · Poisson's ratio: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)Plastic Polypropylene · Thermal conductivity: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)Plastic Polypropylene · Thermal expansion: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Plastic Polypropylene stronger than SLA Resin Elastic 50A?
Plastic Polypropylene is stronger: its yield strength is 33 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (9.71x).
Which is lighter, Plastic Polypropylene or SLA Resin Elastic 50A?
Plastic Polypropylene is lighter: 900 kg/m³ against 1,010 kg/m³ for SLA Resin Elastic 50A.
Which is lighter for the same job, Plastic Polypropylene or SLA Resin Elastic 50A?
For the same stiffness or strength: Plastic Polypropylene is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic Polypropylene
SLA Resin Elastic 50A
Strong rod or tie
lighter
10.9x heavier
Strong beam
lighter
5.11x heavier
Strong panel or plate
lighter
3.5x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).