Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: LyondellBasell, Cleveland-Cliffs, INEOS Olefins & Polymers USA
Plastic Polypropylene
LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values
Stainless Steel 17-4PH
Cleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021)
1
Moplen HP501H Product DataLyondellBasellPlastic Polypropylene · Yield strength: typical, tensile stress at yield ISO 527Plastic Polypropylene · Young's modulus (stiffness): typical, tensile modulus ISO 527Plastic Polypropylene · Density: typical, 23 °C ISO 1183-1Plastic Polypropylene · Max service temperature: HDT 0.45 MPa (ISO 75B), unannealed
2
17-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 17-4PH · Yield strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Ultimate tensile strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Elongation at break: typical, transverse, in 2 in. (50.8 mm)Stainless Steel 17-4PH · Young's modulus (stiffness): H 900Stainless Steel 17-4PH · Density: H 900Stainless Steel 17-4PH · Poisson's ratio: H 900 (column)Stainless Steel 17-4PH · Thermal conductivity: at 149 °C (300 °F), H 900Stainless Steel 17-4PH · Thermal expansion: mean, 21–93 °C (70–200 °F), H 900Stainless Steel 17-4PH · Specific heat: mean, 0–100 °C, H 900Stainless Steel 17-4PH · Max service temperature: strength-retention limit (not oxidation)
3
Typical Engineering Properties of PolypropyleneINEOS Olefins & Polymers USAarchived copyPlastic Polypropylene · Poisson's ratio: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)Plastic Polypropylene · Thermal conductivity: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)Plastic Polypropylene · Thermal expansion: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic Polypropylene stronger than Stainless Steel 17-4PH?
Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against 33 MPa for Plastic Polypropylene (38.6x).
Which is lighter, Plastic Polypropylene or Stainless Steel 17-4PH?
Plastic Polypropylene is lighter: 900 kg/m³ against 7,800 kg/m³ for Stainless Steel 17-4PH.
Which is stiffer, Plastic Polypropylene or Stainless Steel 17-4PH?
Stainless Steel 17-4PH is stiffer: Young's modulus 197 GPa against 1.45 GPa for Plastic Polypropylene, so the same part in Stainless Steel 17-4PH deflects less under the same load.
Which is lighter for the same job, Plastic Polypropylene or Stainless Steel 17-4PH?
For the same stiffness or strength: Plastic Polypropylene is lighter for a stiff panel or plate, strong panel or plate; Stainless Steel 17-4PH is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam.
Part that must be
Plastic Polypropylene
Stainless Steel 17-4PH
Stiff rod or tie (tension)
15.7x heavier
lighter
Stiff beam (bending)
34% heavier
lighter
Stiff panel or plate
lighter
1.69x heavier
Strong rod or tie
4.46x heavier
lighter
Strong beam
32% heavier
lighter
Strong panel or plate
lighter
39% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Plastic Polypropylene or Stainless Steel 17-4PH?
Stainless Steel 17-4PH conducts heat better: 17.9 W/m·K against 0.195 W/m·K for Plastic Polypropylene.
Which expands less with temperature?
Stainless Steel 17-4PH expands less: 10.8 µm/m·K against 90 µm/m·K for Plastic Polypropylene.