| Mechanical | ||
| Yield strength | 1,207MPasourcetypical, 1.0 in. hot-rolled bar, 0.2% offset | 1,275MPasourcetypical, transverse, sheet/strip |
| Ultimate tensile strength | 1,389MPasourcetypical, 1.0 in. bar | 1,379MPasourcetypical, transverse, sheet/strip |
| Elongation at break | 20%sourcetypical, 1.0 in. bar | 9%sourcetypical, transverse, in 2 in. (50.8 mm) |
| Young's modulus (stiffness) | 200GPasourcetypical, 21 °C, annealed + aged | 197GPasourceH 900 |
| Density | 8,221kg/m³sourcenominal, annealed and aged | 7,800kg/m³sourceH 900 |
| Strength to weight | 147kN·m/kg | 163kN·m/kg11% higher |
| Stiffness to weight | 24.3MN·m/kg | 25.3MN·m/kg4% higher |
| Poisson's ratio | 0.294sourcetypical, 21 °C, annealed + aged | 0.272sourceH 900 (column) |
| Shear modulus | 77.3GPa | 77.4GPa |
| Bulk modulus | 162GPa | 144GPa |
| Speed of sound | 4,932m/s | 5,026m/s |
| Thermal | ||
| Thermal conductivity | 11.4W/m·Ksourcetypical, 21 °C, annealed + aged (calculated from resistivity per footnote a) | 17.9W/m·Ksourceat 149 °C (300 °F), H 900 |
| Thermal expansion | 13.2µm/m·Ksourcetypical, mean 21-93 °C, annealed + aged | 10.8µm/m·Ksourcemean, 21–93 °C (70–200 °F), H 900 |
| 100 mm part over a 50 °C swing | 66µm growth | 54µm growth22% less |
| Specific heat | 435J/kg·Ksourcetypical, 21 °C | 460J/kg·Ksourcemean, 0–100 °C, H 900 |
| Heats up and cools (diffusivity) | 3.19mm²/s | 4.99mm²/s1.56x faster |
| Thermal shock resistance | 3,680W/m | 7,809W/m2.12x more resistant |
| Melting point | 1,260–1,336°Csourcemelting range | not sourced |
| Max service temperature | 704°Csourceupper use temperature stated by producer | 316°Csourcestrength-retention limit (not oxidation) |
| Values for | INCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical values | Cleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021) |
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Is Nickel Inconel 718 stronger than Stainless Steel 17-4PH?
Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against 1,207 MPa for Nickel Inconel 718 (6%).
Which is lighter, Nickel Inconel 718 or Stainless Steel 17-4PH?
Stainless Steel 17-4PH is lighter: 7,800 kg/m³ against 8,221 kg/m³ for Nickel Inconel 718.
Which is stiffer, Nickel Inconel 718 or Stainless Steel 17-4PH?
Nickel Inconel 718 is stiffer: Young's modulus 200 GPa against 197 GPa for Stainless Steel 17-4PH, so the same part in Nickel Inconel 718 deflects less under the same load.
Which is lighter for the same job, Nickel Inconel 718 or Stainless Steel 17-4PH?
For the same stiffness or strength: Stainless Steel 17-4PH is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
| Part that must be | Nickel Inconel 718 | Stainless Steel 17-4PH |
|---|---|---|
| Stiff rod or tie (tension) | 4% heavier | lighter |
| Stiff beam (bending) | 5% heavier | lighter |
| Stiff panel or plate | 5% heavier | lighter |
| Strong rod or tie | 11% heavier | lighter |
| Strong beam | 9% heavier | lighter |
| Strong panel or plate | 8% heavier | lighter |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which conducts heat better, Nickel Inconel 718 or Stainless Steel 17-4PH?
Stainless Steel 17-4PH conducts heat better: 17.9 W/m·K against 11.4 W/m·K for Nickel Inconel 718.
Which expands less with temperature?
Stainless Steel 17-4PH expands less: 10.8 µm/m·K against 13.2 µm/m·K for Nickel Inconel 718.
Among 59 materials
Related comparisons
- Nickel Inconel 718 vs. Steel AISI 4340
- Nickel Inconel 718 vs. DMLS 17-4PH Stainless Steel
- Nickel Inconel 718 vs. Steel AISI 1045
- Nickel Inconel 718 vs. DMLS 316L Stainless Steel
- Stainless Steel 17-4PH vs. Steel AISI 4340
- Stainless Steel 17-4PH vs. DMLS 17-4PH Stainless Steel
- Stainless Steel 17-4PH vs. DMLS Ti-6Al-4V ELI Titanium
- Stainless Steel 17-4PH vs. Titanium