Stainless Steel 17-4PHWrought
TitaniumWrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength1,275MPasourcetypical, transverse, sheet/strip885MPasourcetypical, plate (>0.187 in), annealed, 0.2% offset
Ultimate tensile strength1,379MPasourcetypical, transverse, sheet/strip940MPasourcetypical, plate, annealed
Elongation at break9%sourcetypical, transverse, in 2 in. (50.8 mm)16%sourcetypical, in 2 in., plate annealed
Young's modulus (stiffness)197GPasourceH 900107–122GPasourcetypical range, 20 °C
Density7,800kg/m³sourceH 9004,430kg/m³sourcenominal
Strength to weight163kN·m/kg200kN·m/kg22% higher
Stiffness to weight25.3MN·m/kg25.8MN·m/kg2% higher
Poisson's ratio0.272sourceH 900 (column)0.342sourcemean of TIMET measurements
Shear modulus77.4GPa1.82x stiffer in shear42.7GPa
Bulk modulus144GPa121GPa
Speed of sound5,026m/s5,084m/s
Thermal
Thermal conductivity17.9W/m·Ksourceat 149 °C (300 °F), H 9006.6W/m·Ksourcetypical, 20 °C, mill annealed
Thermal expansion10.8µm/m·Ksourcemean, 21–93 °C (70–200 °F), H 9009µm/m·Ksourcetypical, mean 0-100 °C
100 mm part over a 50 °C swing54µm growth45µm growth20% less
Specific heat460J/kg·Ksourcemean, 0–100 °C, H 900580J/kg·Ksourcetypical, 20 °C
Heats up and cools (diffusivity)4.99mm²/s1.94x faster2.57mm²/s
Thermal shock resistance7,809W/m2.09x more resistant3,730W/m
Melting pointnot sourced1,630–1,650°Csourcemelting range
Max service temperature316°Csourcestrength-retention limit (not oxidation)400°Csourceupper recommended use temperature
Values forCleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021)TIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Stainless Steel 17-4PH stronger than Titanium?

Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against 885 MPa for Titanium (44%).

Which is lighter, Stainless Steel 17-4PH or Titanium?

Titanium is lighter: 4,430 kg/m³ against 7,800 kg/m³ for Stainless Steel 17-4PH.

Which is stiffer, Stainless Steel 17-4PH or Titanium?

Stainless Steel 17-4PH is stiffer: Young's modulus 197 GPa against 115 GPa for Titanium, so the same part in Stainless Steel 17-4PH deflects less under the same load.

Which is lighter for the same job, Stainless Steel 17-4PH or Titanium?

For the same stiffness or strength: Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beStainless Steel 17-4PHTitanium
Stiff rod or tie (tension)2% heavierlighter
Stiff beam (bending)34% heavierlighter
Stiff panel or plate47% heavierlighter
Strong rod or tie22% heavierlighter
Strong beam38% heavierlighter
Strong panel or plate47% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Stainless Steel 17-4PH or Titanium?

Stainless Steel 17-4PH conducts heat better: 17.9 W/m·K against 6.6 W/m·K for Titanium.

Which expands less with temperature?

Titanium expands less: 9 µm/m·K against 10.8 µm/m·K for Stainless Steel 17-4PH.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelStainless Steel 17-4PHTitanium
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Aluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickStainless Steel 17-4PHTitanium
Strength against density