Materials / Compare

Nickel Inconel 718 vs. Steel AISI 1045

Compare Nickel Inconel 718 vs. Steel AISI 1045 strength, stiffness, weight and thermal properties.

Change either side
Nickel Inconel 718Wrought
Steel AISI 1045Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength1,207MPasourcetypical, 1.0 in. hot-rolled bar, 0.2% offset531MPasourceproducer-stated, cold drawn
Ultimate tensile strength1,389MPasourcetypical, 1.0 in. bar627MPasourceproducer-stated, cold drawn
Elongation at break20%sourcetypical, 1.0 in. bar12%sourcein 2 in (50.8 mm)
Young's modulus (stiffness)200GPasourcetypical, 21 °C, annealed + aged210GPasourcetypical
Density8,221kg/m³sourcenominal, annealed and aged7,800kg/m³sourcetypical
Strength to weight147kN·m/kg2.16x higher68.1kN·m/kg
Stiffness to weight24.3MN·m/kg26.9MN·m/kg11% higher
Poisson's ratio0.294sourcetypical, 21 °C, annealed + aged0.3sourcetypical
Shear modulus77.3GPa80.8GPa5% stiffer in shear
Bulk modulus162GPa175GPa
Speed of sound4,932m/s5,189m/s
Thermal
Thermal conductivity11.4W/m·Ksourcetypical, 21 °C, annealed + aged (calculated from resistivity per footnote a)40–45W/m·Ksourcetypical range, ambient
Thermal expansion13.2µm/m·Ksourcetypical, mean 21-93 °C, annealed + aged12µm/m·Ksourcetypical, mean 20-300 °C
100 mm part over a 50 °C swing66µm growth60µm growth10% less
Specific heat435J/kg·Ksourcetypical, 21 °C460–480J/kg·Ksourcetypical range, 50/100 °C
Heats up and cools (diffusivity)3.19mm²/s11.6mm²/s3.64x faster
Thermal shock resistance3,680W/m6,269W/m1.7x more resistant
Melting point1,260–1,336°Csourcemelting rangenot sourced
Max service temperature704°Csourceupper use temperature stated by producernot sourced
Values forINCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical valuesAISI 1045 cold drawn bar (Niagara LaSalle) for mechanical; Ovako C45 (lists 'SAE 1045' as a similar designation) for physical constants

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Nickel Inconel 718 stronger than Steel AISI 1045?

Nickel Inconel 718 is stronger: its yield strength is 1,207 MPa against 531 MPa for Steel AISI 1045 (2.27x).

Which is lighter, Nickel Inconel 718 or Steel AISI 1045?

Steel AISI 1045 is lighter: 7,800 kg/m³ against 8,221 kg/m³ for Nickel Inconel 718.

Which is stiffer, Nickel Inconel 718 or Steel AISI 1045?

Steel AISI 1045 is stiffer: Young's modulus 210 GPa against 200 GPa for Nickel Inconel 718, so the same part in Steel AISI 1045 deflects less under the same load.

Which is lighter for the same job, Nickel Inconel 718 or Steel AISI 1045?

For the same stiffness or strength: Nickel Inconel 718 is lighter for a strong rod or tie, strong beam, strong panel or plate; Steel AISI 1045 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beNickel Inconel 718Steel AISI 1045
Stiff rod or tie (tension)11% heavierlighter
Stiff beam (bending)8% heavierlighter
Stiff panel or plate7% heavierlighter
Strong rod or tielighter2.16x heavier
Strong beamlighter1.64x heavier
Strong panel or platelighter43% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Nickel Inconel 718 or Steel AISI 1045?

Steel AISI 1045 conducts heat better: 42.5 W/m·K against 11.4 W/m·K for Nickel Inconel 718.

Which expands less with temperature?

Steel AISI 1045 expands less: 12 µm/m·K against 13.2 µm/m·K for Nickel Inconel 718.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelNickel Inconel 718Steel AISI 1045
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickNickel Inconel 718Steel AISI 1045
Strength against density

Related comparisons