Plastic POM/Acetal vs. Stainless Steel 303
Compare Plastic POM/Acetal vs. Stainless Steel 303 strength, stiffness, weight and thermal properties.
| Mechanical | Plastic POM/Acetal | Stainless Steel 303 |
|---|---|---|
| Yield strength | 69MPa1 | Outokumpu typical275MPa23.99x stronger |
| Ultimate tensile strength | 69MPa1 | Outokumpu typical585MPa28.48x stronger |
| Compressive strength | 124MPa1 | not sourced |
| Flexural strength | 99MPa1 | not sourced |
| Elongation at break | 75%12.14x more ductile | Outokumpu typical35%2 |
| Young's modulus (stiffness) | 2.8GPa1 | at RT200GPa271.4x stiffer |
| Density | 1,420kg/m³35.56x lighter | at RT7,900kg/m³2 |
| Strength to weight | 48.6kN·m/kg40% higher | 34.8kN·m/kg |
| Stiffness to weight | 1.97MN·m/kg | 25.3MN·m/kg12.8x higher |
| Poisson's ratio | 0.351 | design value0.34 |
| Shear modulus | 1.04GPa | 76.9GPa74.2x stiffer in shear |
| Bulk modulus | 3.11GPa | 167GPa53.6x higher |
| Speed of sound | 1,404m/s | 5,032m/s3.58x faster |
| Thermal | Plastic POM/Acetal | Stainless Steel 303 |
|---|---|---|
| Thermal conductivity | 0.4W/m·K1 | at RT15W/m·K237.5x more heat through a fin |
| Thermal expansion | mean122µm/m·K1 | mean16µm/m·K27.63x less |
| 100 mm part over a 50 °C swing | 610µm growth | 80µm growth7.63x less |
| Specific heat | average -18 to 100 °C1,465J/kg·K12.93x higher | at RT500J/kg·K2 |
| Heats up and cools (diffusivity) | 0.192mm²/s | 3.8mm²/s19.7x faster |
| Thermal shock resistance | 52.5W/m | 902W/m17.2x more resistant |
| Melting point | 175°C1 | not sourced |
| Max service temperature | HDT 1.8 MPa125°C1 | continuous871°C5 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources5 documents: DuPont, Outokumpu, Steel Construction Institute, Carpenter Technology
- Plastic POM/Acetal
- DuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.com
- Stainless Steel 303
- 1.4305 / UNS S30300, Outokumpu typical values (hot rolled, solution annealed) from 'Steel Grades, Properties and Global Standards'; max service from Carpenter CarTech 303 datasheet
- 1Delrin Acetal Resin Design Guide, Module IIIDuPontarchived copyPlastic POM/Acetal · Yield strength: typical (single ASTM D638 tensile strength)Plastic POM/Acetal · Ultimate tensile strength: typicalPlastic POM/Acetal · Compressive strength: compressive stress at 10% deformationPlastic POM/Acetal · Flexural strength: flexural yield strength, typicalPlastic POM/Acetal · Elongation at break: typicalPlastic POM/Acetal · Young's modulus (stiffness): typicalPlastic POM/Acetal · Poisson's ratio: typicalPlastic POM/Acetal · Thermal conductivity: typicalPlastic POM/Acetal · Thermal expansion: mean, 29 to 60 °CPlastic POM/Acetal · Specific heat: average -18 to 100 °C, Delrin acetal resins (not grade-specific)Plastic POM/Acetal · Melting point: crystalline melting pointPlastic POM/Acetal · Max service temperature: HDT 1.8 MPa (annealed)
- 2Steel Grades, Properties and Global StandardsOutokumpuarchived copyStainless Steel 303 · Yield strength: Outokumpu typical (product P = hot rolled plate, transverse)Stainless Steel 303 · Ultimate tensile strength: Outokumpu typicalStainless Steel 303 · Elongation at break: Outokumpu typical, A5Stainless Steel 303 · Young's modulus (stiffness): at RT (Table 12)Stainless Steel 303 · Density: at RTStainless Steel 303 · Thermal conductivity: at RTStainless Steel 303 · Thermal expansion: mean, 20–100 °CStainless Steel 303 · Specific heat: at RT
- 3Delrin 100 Product Data SheetDuPontPlastic POM/Acetal · Density: typical (DuPont product information for Delrin 100 NC010; 'The data listed here fall within the normal range of product properties')
- 4Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 303 · Poisson's ratio: design value (structural stainless steels)
- 5Carpenter Stainless Type 303 Data SheetCarpenter Technologyarchived copyStainless Steel 303 · Max service temperature: continuous, scaling limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic POM/Acetal stronger than Stainless Steel 303?
Stainless Steel 303 is stronger: its yield strength is 275 MPa against 69 MPa for Plastic POM/Acetal (3.99x).
Which is lighter, Plastic POM/Acetal or Stainless Steel 303?
Plastic POM/Acetal is lighter: 1,420 kg/m³ against 7,900 kg/m³ for Stainless Steel 303.
Which is stiffer, Plastic POM/Acetal or Stainless Steel 303?
Stainless Steel 303 is stiffer: Young's modulus 200 GPa against 2.8 GPa for Plastic POM/Acetal, so the same part in Stainless Steel 303 deflects less under the same load.
Which is lighter for the same job, Plastic POM/Acetal or Stainless Steel 303?
For the same stiffness or strength: Plastic POM/Acetal is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 303 is lighter for a stiff rod or tie (tension), stiff beam (bending).
| Part that must be | Plastic POM/Acetal | Stainless Steel 303 |
|---|---|---|
| Stiff rod or tie (tension) | 12.8x heavier | lighter |
| Stiff beam (bending) | 1.52x heavier | lighter |
| Stiff panel or plate | lighter | 34% heavier |
| Strong rod or tie | lighter | 40% heavier |
| Strong beam | lighter | 2.21x heavier |
| Strong panel or plate | lighter | 2.79x heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic POM/Acetal or Stainless Steel 303?
Plastic POM/Acetal stretches further before it breaks: 75% elongation at break against 35% for Stainless Steel 303.
Thermal
Which conducts heat better, Plastic POM/Acetal or Stainless Steel 303?
Stainless Steel 303 conducts heat better: 15 W/m·K against 0.4 W/m·K for Plastic POM/Acetal.
Which expands less with temperature?
Stainless Steel 303 expands less: 16 µm/m·K against 122 µm/m·K for Plastic POM/Acetal.
Related comparisons
- Plastic POM/Acetal vs. SLA Resin Standard
- Plastic POM/Acetal vs. Plastic Polycarbonate
- Plastic POM/Acetal vs. Plastic PMMA
- Plastic POM/Acetal vs. Plastic Nylon
- Stainless Steel 303 vs. Stainless Steel 316
- Stainless Steel 303 vs. Stainless Steel 304
- Stainless Steel 303 vs. Steel AISI 1018
- Stainless Steel 303 vs. Steel