Materials / Compare

Plywood vs. Silicon

Compare Plywood vs. Silicon strength, stiffness, weight and thermal properties.

PlywoodNatural
SiliconGrown single crystal
MechanicalPlywoodSilicon
Yield strengthnot given (tensile used)none (brittle)
Ultimate tensile strengthmodulus of rupture41.4MPa1modulus of rupture130MPa23.14x stronger
Flexural strengthstatic bending MOR41.4MPa1modulus of rupture130MPa2
Elongation at breaknot sourcednone (brittle)
Young's modulus (stiffness)7.45GPa1131GPa217.6x stiffer
Densitynot sourced2,329kg/m³2
Strength to weightnot sourced55.8kN·m/kg
Stiffness to weightnot sourced56.2MN·m/kg
Poisson's rationot sourced0.2212
Shear modulusnot sourced53.6GPa
Bulk modulusnot sourced78.3GPa
Speed of soundnot sourced7,500m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4Ceramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Silicon
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4Ceramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Silicon
Strength against densityHigher and further left: stronger for its weight
ThermalPlywoodSilicon
Thermal conductivity0.12W/m·K3163W/m·K2
Thermal expansionbase material3.1–4.5µm/m·K42.62µm/m·K2
100 mm part over a 50 °C swing19µm growth13.1µm growth45% less
Specific heatbase material1,700J/kg·K42.32x higher732J/kg·K2
Heats up and cools (diffusivity)not sourced95.6mm²/s
Thermal shock resistancenot sourced48,095W/m
Melting pointnot sourced1,412°C2
Max service temperaturenot sourced300°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4Ceramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Silicon
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4Ceramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30PlywoodSilicon
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA panel to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: USDA Forest Products Laboratory, Korth Kristalle
Plywood
Douglas-fir plywood sheathing (construction plywood per PS 1), static bending properties from USDA FPL Wood Handbook FPL-GTR-282 Ch. 12 Table 12-2 (Biblis 2000)
Silicon
Synthetic single-crystal silicon (cubic, diamond structure), Korth Kristalle (crystal grower) material data; Korth usually supplies Floating Zone (FZ) material, Czochralski (Cz) also offered. Silicon is elastically anisotropic; the producer quotes one modulus and the solver is isotropic.
  1. 1
    Wood Handbook (FPL-GTR-282), Chapter 12: Mechanical Properties of Wood-Based Composite MaterialsUSDA Forest Products LaboratoryPlywood · Ultimate tensile strength: modulus of rupture (no direct tensile value)Plywood · Flexural strength: static bending MOR (Douglas-fir); range 33.72-42.61 across speciesPlywood · Young's modulus (stiffness): static bending MOE of the panel (Douglas-fir); range 6.96-8.55 across species
  2. 2
    Si: SiliconKorth Kristallearchived copySilicon · Ultimate tensile strength: modulus of rupture (bending fracture stress); brittle, no yield pointSilicon · Flexural strength: modulus of ruptureSilicon · Young's modulus (stiffness): typical (single quoted value of an anisotropic crystal)Silicon · Density: typicalSilicon · Poisson's ratio: typicalSilicon · Thermal conductivity: typical at 313 K (40 °C)Silicon · Thermal expansion: typical at 300 KSilicon · Specific heat: typicalSilicon · Melting point: typicalSilicon · Max service temperature: producer's maximum application temperature (optical components)
  3. 3
    Thermal Properties of Wood and Wood Panel Products for Use in Buildings (1988)USDA Forest Products Laboratoryarchived copyPlywood · Thermal conductivity: APA-recommended design value (Douglas-fir plywood), as reported by FPL/ORNL
  4. 4
    Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryPlywood · Thermal expansion: base material: solid wood parallel to grain, ovendry, range across speciesPlywood · Specific heat: base material: solid wood (all species), 12% MC, 27 C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Plywood stronger than Silicon?

Silicon is stronger: its tensile strength is 130 MPa against 41.4 MPa for Plywood (3.14x).

Which is stiffer, Plywood or Silicon?

Silicon is stiffer: Young's modulus 131 GPa against 7.45 GPa for Plywood, so the same part in Silicon deflects less under the same load.

Thermal

Which conducts heat better, Plywood or Silicon?

Silicon conducts heat better: 163 W/m·K against 0.12 W/m·K for Plywood.

Which expands less with temperature?

Silicon expands less: 2.62 µm/m·K against 3.8 µm/m·K for Plywood.

Related comparisons