Materials / Compare

SLA Resin Standard vs. Plastic TPU

Compare SLA Resin Standard vs. Plastic TPU strength, stiffness, weight and thermal properties.

Change either side
SLA Resin Standard3D printed (SLA resin)
Plastic TPU3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength60MPasourcetypical23.7MPasourcetypical, stress at break
Flexural strength105MPasourcetypical25.6x stronger in bending4.1MPasourcetypical
Elongation at break8%sourcetypicalnot sourced
Young's modulus (stiffness)2.75GPasourcetypical41x stiffer0.067GPasourcetypical
Densitynot sourced1,220kg/m³sourcetypical
Strength to weightnot sourced19.4kN·m/kg
Stiffness to weightnot sourced0.0549MN·m/kg
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourced234m/s
Thermal
Thermal conductivitynot sourcednot sourced
Thermal expansionnot sourcednot sourced
100 mm part over a 50 °C swingnot sourcednot sourced
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourcednot sourced
Melting pointnot sourced217°Csourcetypical
Max service temperature59°CsourceHDT 1.8 MPa50.3°CsourceHDT 0.455 MPa (printed specimens)
Values forFormlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.Ultimaker TPU 95A, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 29, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Standard and Plastic TPU are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is SLA Resin Standard stronger than Plastic TPU?

SLA Resin Standard is stronger: its tensile strength is 60 MPa against 23.7 MPa for Plastic TPU (2.53x).

Which is stiffer, SLA Resin Standard or Plastic TPU?

SLA Resin Standard is stiffer: Young's modulus 2.75 GPa against 0.067 GPa for Plastic TPU, so the same part in SLA Resin Standard deflects less under the same load.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic TPU
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic TPU
Strength against density