Materials / Compare

Rubber vs. Steel AISI 1045

Compare Rubber vs. Steel AISI 1045 strength, stiffness, weight and thermal properties.

Change either side
RubberBulk polymer (molded or machined)
Steel AISI 1045Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)531MPasourceproducer-stated, cold drawn
Ultimate tensile strength23MPasourcetypical627MPasourceproducer-stated, cold drawn
Elongation at break830%sourcetypical12%sourcein 2 in (50.8 mm)
Young's modulus (stiffness)not sourced210GPasourcetypical
Density960kg/m³sourcetypical (specific gravity)7,800kg/m³sourcetypical
Strength to weight24kN·m/kg68.1kN·m/kg2.84x higher
Stiffness to weightnot sourced26.9MN·m/kg
Poisson's ratio0.5sourcegovernment (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).0.3sourcetypical
Shear modulusnot sourced80.8GPa
Bulk modulusnot sourced175GPa
Speed of soundnot sourced5,189m/s
Thermal
Thermal conductivity0.151W/m·Ksourcegovernment selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C40–45W/m·Ksourcetypical range, ambient
Thermal expansionnot sourced12µm/m·Ksourcetypical, mean 20-300 °C
100 mm part over a 50 °C swingnot sourced60µm growth
Specific heat1,881J/kg·Ksourcegovernment (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C460–480J/kg·Ksourcetypical range, 50/100 °C
Heats up and cools (diffusivity)0.0836mm²/s11.6mm²/s139x faster
Thermal shock resistancenot sourced6,269W/m
Max service temperature70°Csourcecontinuous use operating rangenot sourced
Values forWeir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305AISI 1045 cold drawn bar (Niagara LaSalle) for mechanical; Ovako C45 (lists 'SAE 1045' as a similar designation) for physical constants

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Rubber stronger than Steel AISI 1045?

Steel AISI 1045 is stronger: its yield strength is 531 MPa against tensile strength 23 MPa for Rubber (23.1x).

Which is lighter, Rubber or Steel AISI 1045?

Rubber is lighter: 960 kg/m³ against 7,800 kg/m³ for Steel AISI 1045.

Which is lighter for the same job, Rubber or Steel AISI 1045?

For the same stiffness or strength: Rubber is lighter for a strong panel or plate; Steel AISI 1045 is lighter for a strong rod or tie.

Part that must beRubberSteel AISI 1045
Strong rod or tie2.84x heavierlighter
Strong beamabout equalabout equal
Strong panel or platelighter1.69x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Rubber or Steel AISI 1045?

Steel AISI 1045 conducts heat better: 42.5 W/m·K against 0.151 W/m·K for Rubber.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelSteel AISI 1045
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickRubberSteel AISI 1045
Strength against density

Related comparisons