Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Carpenter Technology, Weir Minerals, U.S. Department of Defense, National Institute of Standards and Technology, Defense Technical Information Center
Linatex Premium Rubber Spec Sheet (WMD0118, 2023)Weir MineralsRubber · Ultimate tensile strength: typicalRubber · Elongation at break: typicalRubber · Density: typical (specific gravity)Rubber · Max service temperature: continuous use operating range
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)
4
Compressibility of Natural Rubber at Pressures Below 500 kg/cm², J. Res. NBS 68A (1964)National Institute of Standards and Technologyarchived copyRubber · Poisson's ratio: government (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation (0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).)Rubber · Specific heat: government (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
5
Thermal Conductivity of Soft Vulcanized Natural Rubber: Selected Values (AD 643325)Defense Technical Information Centerarchived copyRubber · Thermal conductivity: government selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Rubber stronger than Steel AISI 4340?
Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against tensile strength 23 MPa for Rubber (45x).
Which is lighter, Rubber or Steel AISI 4340?
Rubber is lighter: 960 kg/m³ against 7,840 kg/m³ for Steel AISI 4340.
Which is lighter for the same job, Rubber or Steel AISI 4340?
For the same stiffness or strength: Rubber is lighter for a strong panel or plate; Steel AISI 4340 is lighter for a strong rod or tie, strong beam.
Part that must be
Rubber
Steel AISI 4340
Strong rod or tie
5.51x heavier
lighter
Strong beam
1.55x heavier
lighter
Strong panel or plate
lighter
22% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Rubber or Steel AISI 4340?
Rubber stretches further before it breaks: 830% elongation at break against 18% for Steel AISI 4340.
Thermal
Which conducts heat better, Rubber or Steel AISI 4340?
Steel AISI 4340 conducts heat better: 37.5 W/m·K against 0.151 W/m·K for Rubber.