Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Formlabs, American Institute of Steel Construction, bauforumstahl (ArcelorMittal), Ovako
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
Steel A992
ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel A992 · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel A992 · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel A992 · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
3
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel A992 · Young's modulus (stiffness): design value (AISC 360-16)Steel A992 · Poisson's ratio: design value (AISC 360-16 Commentary)
4
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel A992 · Density: nominal (constructional data)Steel A992 · Thermal conductivity: nominal at 20 °CSteel A992 · Thermal expansion: nominal (constructional data, no temperature range stated)
5
S275JR Steel GradeOvakoSteel A992 · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is SLA Resin Tough 2000 stronger than Steel A992?
Steel A992 is stronger: its yield strength is 385 MPa against 40.4 MPa for SLA Resin Tough 2000 (9.53x).
Which is lighter, SLA Resin Tough 2000 or Steel A992?
SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 7,850 kg/m³ for Steel A992.
Which is stiffer, SLA Resin Tough 2000 or Steel A992?
Steel A992 is stiffer: Young's modulus 200 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Steel A992 deflects less under the same load.
Which is lighter for the same job, SLA Resin Tough 2000 or Steel A992?
For the same stiffness or strength: SLA Resin Tough 2000 is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel A992 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.
Part that must be
SLA Resin Tough 2000
Steel A992
Stiff rod or tie (tension)
15.4x heavier
lighter
Stiff beam (bending)
46% heavier
lighter
Stiff panel or plate
lighter
50% heavier
Strong rod or tie
32% heavier
lighter
Strong beam
lighter
1.6x heavier
Strong panel or plate
lighter
2.33x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, SLA Resin Tough 2000 or Steel A992?
SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 24.2% for Steel A992.
Thermal
Which expands less with temperature?
Steel A992 expands less: 12 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.