Materials / Compare
Stainless Steel 17-4PH vs. Steel AISI 1018
Compare Stainless Steel 17-4PH vs. Steel AISI 1018 strength, stiffness, weight and thermal properties.
| Mechanical | Stainless Steel 17-4PH | Steel AISI 1018 |
|---|---|---|
| Yield strength | 1,275MPa13.43x stronger | producer-stated372MPa2 |
| Ultimate tensile strength | 1,379MPa13.13x stronger | producer-stated441MPa2 |
| Elongation at break | 9%1 | in 2 in15%21.67x more ductile |
| Young's modulus (stiffness) | H 900197GPa1 | base material200GPa3 |
| Density | H 9007,800kg/m³1 | base material7,861kg/m³3 |
| Strength to weight | 163kN·m/kg3.45x higher | 47.3kN·m/kg |
| Stiffness to weight | 25.3MN·m/kg | 25.4MN·m/kg |
| Poisson's ratio | H 9000.2721 | base material0.323 |
| Shear modulus | 77.4GPa2% stiffer in shear | 75.7GPa |
| Bulk modulus | 144GPa | 185GPa29% higher |
| Speed of sound | 5,026m/s | 5,043m/s |
| Thermal | Stainless Steel 17-4PH | Steel AISI 1018 |
|---|---|---|
| Thermal conductivity | at 149 °C17.9W/m·K1 | base material51.9W/m·K3 |
| Thermal expansion | mean10.8µm/m·K1 | base material12µm/m·K4 |
| 100 mm part over a 50 °C swing | 54µm growth11% less | 60µm growth |
| Specific heat | mean460J/kg·K1 | base material486J/kg·K3 |
| Heats up and cools (diffusivity) | 4.99mm²/s | 13.6mm²/s2.72x faster |
| Thermal shock resistance | 7,809W/m43% more resistant | 5,473W/m |
| Max service temperature | 316°C1 | not sourced |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources4 documents: Cleveland-Cliffs, Niagara LaSalle, U.S. Department of Defense, Ovako
- Stainless Steel 17-4PH
- Cleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021)
- Steel AISI 1018
- AISI 1018 cold drawn bar (Niagara LaSalle, cold-finished bar producer)
- 117-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 17-4PH · Yield strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Ultimate tensile strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Elongation at break: typical, transverse, in 2 in. (50.8 mm)Stainless Steel 17-4PH · Young's modulus (stiffness): H 900Stainless Steel 17-4PH · Density: H 900Stainless Steel 17-4PH · Poisson's ratio: H 900 (column)Stainless Steel 17-4PH · Thermal conductivity: at 149 °C (300 °F), H 900Stainless Steel 17-4PH · Thermal expansion: mean, 21–93 °C (70–200 °F), H 900Stainless Steel 17-4PH · Specific heat: mean, 0–100 °C, H 900Stainless Steel 17-4PH · Max service temperature: strength-retention limit (not oxidation)
- 21018 PropertiesNiagara LaSallearchived copySteel AISI 1018 · Yield strength: producer-stated, cold drawnSteel AISI 1018 · Ultimate tensile strength: producer-stated, cold drawnSteel AISI 1018 · Elongation at break: in 2 in (50.8 mm)
- 3MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 1018 · Young's modulus (stiffness): base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Density: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Poisson's ratio: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Thermal conductivity: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Specific heat: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
- 4S275JR Steel GradeOvakoSteel AISI 1018 · Thermal expansion: base material: unalloyed carbon steel, Ovako family table (S275JR, 'none alloyed structural steels', C <= 0.21%); mean 20-300 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Stainless Steel 17-4PH stronger than Steel AISI 1018?
Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against 372 MPa for Steel AISI 1018 (3.43x).
Which is lighter, Stainless Steel 17-4PH or Steel AISI 1018?
Stainless Steel 17-4PH is lighter: 7,800 kg/m³ against 7,861 kg/m³ for Steel AISI 1018.
Which is stiffer, Stainless Steel 17-4PH or Steel AISI 1018?
Steel AISI 1018 is stiffer: Young's modulus 200 GPa against 197 GPa for Stainless Steel 17-4PH, so the same part in Steel AISI 1018 deflects less under the same load.
Which is lighter for the same job, Stainless Steel 17-4PH or Steel AISI 1018?
For the same stiffness or strength: Stainless Steel 17-4PH is lighter for a strong rod or tie, strong beam, strong panel or plate.
| Part that must be | Stainless Steel 17-4PH | Steel AISI 1018 |
|---|---|---|
| Stiff rod or tie (tension) | about equal | about equal |
| Stiff beam (bending) | about equal | about equal |
| Stiff panel or plate | about equal | about equal |
| Strong rod or tie | lighter | 3.45x heavier |
| Strong beam | lighter | 2.29x heavier |
| Strong panel or plate | lighter | 1.87x heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Stainless Steel 17-4PH or Steel AISI 1018?
Steel AISI 1018 stretches further before it breaks: 15% elongation at break against 9% for Stainless Steel 17-4PH.
Thermal
Which conducts heat better, Stainless Steel 17-4PH or Steel AISI 1018?
Steel AISI 1018 conducts heat better: 51.9 W/m·K against 17.9 W/m·K for Stainless Steel 17-4PH.
Which expands less with temperature?
Stainless Steel 17-4PH expands less: 10.8 µm/m·K against 12 µm/m·K for Steel AISI 1018.
Related comparisons
- Stainless Steel 17-4PH vs. Nickel Inconel 718
- Stainless Steel 17-4PH vs. Steel AISI 4340
- Stainless Steel 17-4PH vs. DMLS 17-4PH Stainless Steel
- Stainless Steel 17-4PH vs. DMLS Ti-6Al-4V ELI Titanium
- Steel AISI 1018 vs. Steel
- Steel AISI 1018 vs. Steel A992
- Steel AISI 1018 vs. Stainless Steel 303
- Steel AISI 1018 vs. Stainless Steel 316