Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: ATI, Carpenter Technology, U.S. Department of Defense, Steel Construction Institute
Stainless Steel 316
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)
4
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Stainless Steel 316 stronger than Steel AISI 4340?
Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against 265 MPa for Stainless Steel 316 (3.91x).
Which is lighter, Stainless Steel 316 or Steel AISI 4340?
Steel AISI 4340 is lighter: 7,840 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.
Which is stiffer, Stainless Steel 316 or Steel AISI 4340?
Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 200 GPa for Steel AISI 4340, so the same part in Stainless Steel 316 deflects less under the same load.
Which is lighter for the same job, Stainless Steel 316 or Steel AISI 4340?
For the same stiffness or strength: Steel AISI 4340 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Stainless Steel 316
Steel AISI 4340
Stiff rod or tie (tension)
2% heavier
lighter
Stiff beam (bending)
2% heavier
lighter
Stiff panel or plate
2% heavier
lighter
Strong rod or tie
4x heavier
lighter
Strong beam
2.54x heavier
lighter
Strong panel or plate
2.02x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Stainless Steel 316 or Steel AISI 4340?
Stainless Steel 316 stretches further before it breaks: 61% elongation at break against 18% for Steel AISI 4340.
Thermal
Which conducts heat better, Stainless Steel 316 or Steel AISI 4340?
Steel AISI 4340 conducts heat better: 37.5 W/m·K against 14.6 W/m·K for Stainless Steel 316.
Which expands less with temperature?
Steel AISI 4340 expands less: 11.3 µm/m·K against 16.5 µm/m·K for Stainless Steel 316.