Materials / Compare

Aluminum 7075-T6 vs. Plastic Nylon PA6

Compare Aluminum 7075-T6 vs. Plastic Nylon PA6 strength, stiffness, weight and thermal properties.

Change either side
Aluminum 7075-T6Wrought
Plastic Nylon PA6Bulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength503MPasourcetypical, 0.2% offset, .500 in dia specimen90MPasourcetypical, dry
Ultimate tensile strength572MPasourcetypicalnot sourced
Elongation at break11%sourcetypical, in 4D10%sourcenominal strain at break, dry
Young's modulus (stiffness)71GPasourcetypical3.5GPasourcetypical, dry
Density2,800kg/m³sourcenominal1,130kg/m³sourcetypical
Strength to weight180kN·m/kg2.26x higher79.6kN·m/kg
Stiffness to weight25.4MN·m/kg8.19x higher3.1MN·m/kg
Poisson's ratio0.33sourcetypical (handbook physical constant)0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Shear modulus26.7GPa21.4x stiffer in shear1.25GPa
Bulk modulus69.6GPa5.83GPa
Speed of sound5,036m/s1,760m/s
Thermal
Thermal conductivity130W/m·Ksourcetypical, 20 °C, T6510.33W/m·Ksourcetypical
Thermal expansion23.4µm/m·Ksourcetypical, mean 20-100 °C102µm/m·Ksourcelongitudinal, 23-55 °C
100 mm part over a 50 °C swing117µm growth4.36x less510µm growth
Specific heat960J/kg·Ksourcetypical, at 100 °C1,700J/kg·Ksourcetypical
Heats up and cools (diffusivity)48.4mm²/s282x faster0.172mm²/s
Thermal shock resistance26,370W/m528x more resistant49.9W/m
Melting point532–635°Csourcemelting range220°CsourceDSC
Max service temperaturenot sourced87°CsourceIEC 60216 temperature index, 20000 h
Values for7075-T6/T651, Kaiser Aluminum rod & bar (mechanical) and sheet/coil/plate (physical) typical datasheets; Poisson from MIL-HDBK-5JBASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum 7075-T6 stronger than Plastic Nylon PA6?

Aluminum 7075-T6 is stronger: its yield strength is 503 MPa against 90 MPa for Plastic Nylon PA6 (5.59x).

Which is lighter, Aluminum 7075-T6 or Plastic Nylon PA6?

Plastic Nylon PA6 is lighter: 1,130 kg/m³ against 2,800 kg/m³ for Aluminum 7075-T6.

Which is stiffer, Aluminum 7075-T6 or Plastic Nylon PA6?

Aluminum 7075-T6 is stiffer: Young's modulus 71 GPa against 3.5 GPa for Plastic Nylon PA6, so the same part in Aluminum 7075-T6 deflects less under the same load.

Which is lighter for the same job, Aluminum 7075-T6 or Plastic Nylon PA6?

For the same stiffness or strength: Aluminum 7075-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam; Plastic Nylon PA6 is lighter for a strong panel or plate.

Part that must beAluminum 7075-T6Plastic Nylon PA6
Stiff rod or tie (tension)lighter8.19x heavier
Stiff beam (bending)lighter1.82x heavier
Stiff panel or platelighter10% heavier
Strong rod or tielighter2.26x heavier
Strong beamlighter27% heavier
Strong panel or plate5% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum 7075-T6 or Plastic Nylon PA6?

Aluminum 7075-T6 conducts heat better: 130 W/m·K against 0.33 W/m·K for Plastic Nylon PA6.

Which expands less with temperature?

Aluminum 7075-T6 expands less: 23.4 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 7075-T6Plastic Nylon PA6
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 7075-T6Plastic Nylon PA6
Strength against density