Aluminum 7075-T6 vs. Rubber Compare Aluminum 7075-T6 vs. Rubber strength, stiffness, weight and thermal properties.
Change either side
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless 304 Stainless 316 Stainless 303 Stainless 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall Aluminum 7075-T6 Wrought Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless 304 Stainless 316 Stainless 303 Stainless 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall Rubber Bulk polymer (molded or machined) Try it on a partA bracket to run stress or thermal on, free in your browser Open in LessCAD Open in LessCAD Mechanical Yield strength 503 MPa source typical, 0.2% offset, .500 in dia specimen not given (tensile used) Ultimate tensile strength 572 MPa source typical 24.9x stronger 23 MPa source typical Elongation at break 11 % source typical, in 4D 830 % source typical Young's modulus (stiffness) 71 GPa source typical not sourced Density 2,800 kg/m³ source nominal 960 kg/m³ source typical (specific gravity) Strength to weight 180 kN·m/kg 7.5x higher 24 kN·m/kg Stiffness to weight 25.4 MN·m/kg not sourced Poisson's ratio 0.33 source typical (handbook physical constant) 0.5 source government (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation 0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible). Shear modulus 26.7 GPa not sourced Bulk modulus 69.6 GPa not sourced Speed of sound 5,036 m/s not sourced Thermal Thermal conductivity 130 W/m·K source typical, 20 °C, T651 0.151 W/m·K source government selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C Thermal expansion 23.4 µm/m·K source typical, mean 20-100 °C not sourced 100 mm part over a 50 °C swing 117 µm growth not sourced Specific heat 960 J/kg·K source typical, at 100 °C 1,881 J/kg·K source government (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C Heats up and cools (diffusivity) 48.4 mm²/s 578x faster 0.0836 mm²/s Thermal shock resistance 26,370 W/m not sourced Melting point 532–635 °C source melting range not sourced Max service temperature not sourced 70 °C source continuous use operating range Values for 7075-T6/T651, Kaiser Aluminum rod & bar (mechanical) and sheet/coil/plate (physical) typical datasheets; Poisson from MIL-HDBK-5J Weir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions Is Aluminum 7075-T6 stronger than Rubber? Aluminum 7075-T6 is stronger: its yield strength is 503 MPa against tensile strength 23 MPa for Rubber (21.9x).
Which is lighter, Aluminum 7075-T6 or Rubber? Rubber is lighter: 960 kg/m³ against 2,800 kg/m³ for Aluminum 7075-T6.
Which is lighter for the same job, Aluminum 7075-T6 or Rubber? For the same stiffness or strength: Aluminum 7075-T6 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be Aluminum 7075-T6 Rubber Strong rod or tie lighter 7.5x heavier Strong beam lighter 2.68x heavier Strong panel or plate lighter 1.6x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which conducts heat better, Aluminum 7075-T6 or Rubber? Aluminum 7075-T6 conducts heat better: 130 W/m·K against 0.151 W/m·K for Rubber.
Among 59 materials 1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Aluminum Steel Iron Titanium Steel AISI 1018 Stainless 304 Stainless 316 Aluminum 6061-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless 303 Stainless 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Aluminum 7075-T6 Stiffness against density 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Aluminum Steel Iron Titanium Steel AISI 1018 Stainless 304 Stainless 316 Aluminum 6061-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless 303 Stainless 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick Aluminum 7075-T6 Rubber Strength against density