Aluminum 1100-O vs. Plastic LCP GF30

Compare Aluminum 1100-O vs. Plastic LCP GF30 strength, stiffness, weight and thermal properties.

Aluminum 1100-OWrought
Plastic LCP GF30Bulk polymer (molded or machined)
MechanicalAluminum 1100-OPlastic LCP GF30
Yield strength35MPa1not given (tensile used)
Ultimate tensile strength90MPa1tensile strength115MPa228% stronger
Flexural strengthnot sourced184MPa2
Elongation at break35%123.3x more ductiletensile elongation1.5%2
Young's modulus (stiffness)69GPa16x stiffertensile modulus11.5GPa2
Density2,710kg/m³11,610kg/m³21.68x lighter
Strength to weight12.9kN·m/kg71.4kN·m/kg5.53x higher
Stiffness to weight25.5MN·m/kg3.56x higher7.14MN·m/kg
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound5,046m/s1.89x faster2,673m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Aluminum 1100-OPlastic LCP GF30
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Aluminum 1100-OPlastic LCP GF30
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 1100-OPlastic LCP GF30
Thermal conductivity222W/m·K1444x more heat through a finhot disk0.5W/m·K2
Thermal expansion23.6µm/m·K1flow direction20µm/m·K218% less
100 mm part over a 50 °C swing118µm growth100µm growth18% less
Specific heatbase material901J/kg·K3ASTM E1269839J/kg·K2
Heats up and cools (diffusivity)90.9mm²/s246x faster0.37mm²/s
Thermal shock resistancenot sourcednot sourced
Melting pointmelting range640–655°C1not sourced
Max service temperaturenot sourcedHDT 1.8 MPa288°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Aluminum 1100-OPlastic LCP GF30
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Aluminum 1100-OPlastic LCP GF30
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Kaiser Aluminum, Sumitomo Chemical, Hydro
Aluminum 1100-O
1100-O (annealed) commercially pure aluminium, Kaiser Aluminum Tube & Pipe Alloy 1100 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-1050A (99.5% Al) extruded-products datasheet (10/2018).
Plastic LCP GF30
Sumitomo Chemical SUMIKASUPER LCP E6006L (30% glass fibre; high strength, low shrinkage); SUMIKASUPER LCP Technical Note, Version 04 / Nov. 2023, typical values.
  1. 1
    Alloy 1100 Tube & Pipe Technical Data, Rev. 05/06Kaiser Aluminumarchived copyAluminum 1100-O · Yield strength: typical, O, 0.0625 in specimenAluminum 1100-O · Ultimate tensile strength: typical, OAluminum 1100-O · Elongation at break: typical, O, in 4DAluminum 1100-O · Young's modulus (stiffness): typicalAluminum 1100-O · Density: nominal, 20 °CAluminum 1100-O · Thermal conductivity: typical, O, 20 °CAluminum 1100-O · Thermal expansion: typical, mean 20-100 °CAluminum 1100-O · Melting point: melting range
  2. 2
    SUMIKASUPER LCP Technical Note, Version 04 (2023)Sumitomo Chemicalarchived copyPlastic LCP GF30 · Ultimate tensile strength: tensile strength (ISO 527)Plastic LCP GF30 · Flexural strength: typical (ISO 178)Plastic LCP GF30 · Elongation at break: tensile elongation (ISO 527)Plastic LCP GF30 · Young's modulus (stiffness): tensile modulus (ISO 527)Plastic LCP GF30 · Density: typicalPlastic LCP GF30 · Thermal conductivity: hot disk (ISO 22007-2), temperature not statedPlastic LCP GF30 · Thermal expansion: flow direction (MD), mean 50-150 °CPlastic LCP GF30 · Specific heat: ASTM E1269, temperature not statedPlastic LCP GF30 · Max service temperature: HDT 1.8 MPa (ISO 75)
  3. 3
    Technical Datasheet, Extruded Products: Alloy EN AW-1050AHydroAluminum 1100-O · Specific heat: base material: commercially pure aluminium EN AW-1050A (Hydro), 20 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 1100-O stronger than Plastic LCP GF30?

Plastic LCP GF30 is stronger: its tensile strength is 115 MPa against yield strength 35 MPa for Aluminum 1100-O (3.29x).

Which is lighter, Aluminum 1100-O or Plastic LCP GF30?

Plastic LCP GF30 is lighter: 1,610 kg/m³ against 2,710 kg/m³ for Aluminum 1100-O.

Which is stiffer, Aluminum 1100-O or Plastic LCP GF30?

Aluminum 1100-O is stiffer: Young's modulus 69 GPa against 11.5 GPa for Plastic LCP GF30, so the same part in Aluminum 1100-O deflects less under the same load.

Which is lighter for the same job, Aluminum 1100-O or Plastic LCP GF30?

For the same stiffness or strength: Aluminum 1100-O is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Plastic LCP GF30 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 1100-OPlastic LCP GF30
Stiff rod or tie (tension)lighter3.56x heavier
Stiff beam (bending)lighter46% heavier
Stiff panel or platelighter8% heavier
Strong rod or tie5.53x heavierlighter
Strong beam3.72x heavierlighter
Strong panel or plate3.05x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 1100-O or Plastic LCP GF30?

Aluminum 1100-O stretches further before it breaks: 35% elongation at break against 1.5% for Plastic LCP GF30.

Thermal

Which conducts heat better, Aluminum 1100-O or Plastic LCP GF30?

Aluminum 1100-O conducts heat better: 222 W/m·K against 0.5 W/m·K for Plastic LCP GF30.

Which expands less with temperature?

Plastic LCP GF30 expands less: 20 µm/m·K against 23.6 µm/m·K for Aluminum 1100-O.