Aluminum 1100-O vs. Plywood

Compare Aluminum 1100-O vs. Plywood strength, stiffness, weight and thermal properties.

Aluminum 1100-OWrought
PlywoodNatural
MechanicalAluminum 1100-OPlywood
Yield strength35MPa1not given (tensile used)
Ultimate tensile strength90MPa1modulus of rupture41.4MPa2
Flexural strengthnot sourcedstatic bending MOR41.4MPa2
Elongation at break35%1not sourced
Young's modulus (stiffness)69GPa19.26x stiffer7.45GPa2
Density2,710kg/m³1not sourced
Strength to weight12.9kN·m/kgnot sourced
Stiffness to weight25.5MN·m/kgnot sourced
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound5,046m/snot sourced
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-O
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-O
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 1100-OPlywood
Thermal conductivity222W/m·K10.12W/m·K3
Thermal expansion23.6µm/m·K1base material3.1–4.5µm/m·K4
100 mm part over a 50 °C swing118µm growth19µm growth6.21x less
Specific heatbase material901J/kg·K5base material1,700J/kg·K41.89x higher
Heats up and cools (diffusivity)90.9mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Melting pointmelting range640–655°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-O
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-OPlywood
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA panel to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Kaiser Aluminum, USDA Forest Products Laboratory, Hydro
Aluminum 1100-O
1100-O (annealed) commercially pure aluminium, Kaiser Aluminum Tube & Pipe Alloy 1100 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-1050A (99.5% Al) extruded-products datasheet (10/2018).
Plywood
Douglas-fir plywood sheathing (construction plywood per PS 1), static bending properties from USDA FPL Wood Handbook FPL-GTR-282 Ch. 12 Table 12-2 (Biblis 2000)
  1. 1
    Alloy 1100 Tube & Pipe Technical Data, Rev. 05/06Kaiser Aluminumarchived copyAluminum 1100-O · Yield strength: typical, O, 0.0625 in specimenAluminum 1100-O · Ultimate tensile strength: typical, OAluminum 1100-O · Elongation at break: typical, O, in 4DAluminum 1100-O · Young's modulus (stiffness): typicalAluminum 1100-O · Density: nominal, 20 °CAluminum 1100-O · Thermal conductivity: typical, O, 20 °CAluminum 1100-O · Thermal expansion: typical, mean 20-100 °CAluminum 1100-O · Melting point: melting range
  2. 2
    Wood Handbook (FPL-GTR-282), Chapter 12: Mechanical Properties of Wood-Based Composite MaterialsUSDA Forest Products LaboratoryPlywood · Ultimate tensile strength: modulus of rupture (no direct tensile value)Plywood · Flexural strength: static bending MOR (Douglas-fir); range 33.72-42.61 across speciesPlywood · Young's modulus (stiffness): static bending MOE of the panel (Douglas-fir); range 6.96-8.55 across species
  3. 3
    Thermal Properties of Wood and Wood Panel Products for Use in Buildings (1988)USDA Forest Products Laboratoryarchived copyPlywood · Thermal conductivity: APA-recommended design value (Douglas-fir plywood), as reported by FPL/ORNL
  4. 4
    Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryPlywood · Thermal expansion: base material: solid wood parallel to grain, ovendry, range across speciesPlywood · Specific heat: base material: solid wood (all species), 12% MC, 27 C
  5. 5
    Technical Datasheet, Extruded Products: Alloy EN AW-1050AHydroAluminum 1100-O · Specific heat: base material: commercially pure aluminium EN AW-1050A (Hydro), 20 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 1100-O stronger than Plywood?

Plywood is stronger: its tensile strength is 41.4 MPa against yield strength 35 MPa for Aluminum 1100-O (18%).

Which is stiffer, Aluminum 1100-O or Plywood?

Aluminum 1100-O is stiffer: Young's modulus 69 GPa against 7.45 GPa for Plywood, so the same part in Aluminum 1100-O deflects less under the same load.

Thermal

Which conducts heat better, Aluminum 1100-O or Plywood?

Aluminum 1100-O conducts heat better: 222 W/m·K against 0.12 W/m·K for Plywood.

Which expands less with temperature?

Plywood expands less: 3.8 µm/m·K against 23.6 µm/m·K for Aluminum 1100-O.