MechanicalAluminum 2024-T351Plastic Nylon PA66
Yield strength324MPa13.81x stronger85MPa2
Ultimate tensile strength469MPa1not stated (yield given)
Elongation at break19%130%21.58x more ductile
Young's modulus (stiffness)73.1GPa124.4x stiffer3GPa2
Density2,770kg/m³11,130kg/m³22.45x lighter
Strength to weight117kN·m/kg1.55x higher75.2kN·m/kg
Stiffness to weight26.4MN·m/kg9.94x higher2.65MN·m/kg
Poisson's ratio0.333base material0.44
Shear modulus27.5GPa25.6x stiffer in shear1.07GPa
Bulk modulus71.7GPa14.3x higher5GPa
Speed of sound5,137m/s3.15x faster1,629m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 2024-T351Plastic Nylon PA66
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 2024-T351Plastic Nylon PA66
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 2024-T351Plastic Nylon PA66
Thermal conductivity120W/m·K1364x more heat through a fin0.33W/m·K2
Thermal expansion22.9µm/m·K14.28x lesslongitudinal98µm/m·K2
100 mm part over a 50 °C swing115µm growth4.28x less490µm growth
Specific heat875J/kg·K11,700J/kg·K21.94x higher
Heats up and cools (diffusivity)49.5mm²/s288x faster0.172mm²/s
Thermal shock resistance15,561W/m272x more resistant57.2W/m
Melting pointmelting range502–638°C1DSC260°C2
Max service temperaturenot sourced101°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 2024-T351Plastic Nylon PA66
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 2024-T351Plastic Nylon PA66
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Kaiser Aluminum, BASF, U.S. Department of Defense, Covestro
Aluminum 2024-T351
2024-T4/T351, Kaiser Aluminum sheet, coil & plate typical datasheet; Poisson from MIL-HDBK-5J
Plastic Nylon PA66
BASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)
  1. 1
    Alloy 2024 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 2024-T351 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 2024-T351 · Ultimate tensile strength: typicalAluminum 2024-T351 · Elongation at break: typical, in 4DAluminum 2024-T351 · Young's modulus (stiffness): typicalAluminum 2024-T351 · Density: nominalAluminum 2024-T351 · Thermal conductivity: typical, 20 °CAluminum 2024-T351 · Thermal expansion: typical, mean 20-100 °CAluminum 2024-T351 · Specific heat: typical, at 100 °CAluminum 2024-T351 · Melting point: melting range
  2. 2
    Ultramid A3K Product InformationBASFPlastic Nylon PA66 · Yield strength: typical, dryPlastic Nylon PA66 · Elongation at break: nominal strain at break, dryPlastic Nylon PA66 · Young's modulus (stiffness): typical, dryPlastic Nylon PA66 · Density: typicalPlastic Nylon PA66 · Thermal conductivity: typicalPlastic Nylon PA66 · Thermal expansion: longitudinal, 23-55 °CPlastic Nylon PA66 · Specific heat: typicalPlastic Nylon PA66 · Melting point: DSCPlastic Nylon PA66 · Max service temperature: IEC 60216 temperature index, 20000 h
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 2024-T351 · Poisson's ratio: typical (handbook physical constant), all tempers
  4. 4
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon PA66 · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 2024-T351 stronger than Plastic Nylon PA66?

Aluminum 2024-T351 is stronger: its yield strength is 324 MPa against 85 MPa for Plastic Nylon PA66 (3.81x).

Which is lighter, Aluminum 2024-T351 or Plastic Nylon PA66?

Plastic Nylon PA66 is lighter: 1,130 kg/m³ against 2,770 kg/m³ for Aluminum 2024-T351.

Which is stiffer, Aluminum 2024-T351 or Plastic Nylon PA66?

Aluminum 2024-T351 is stiffer: Young's modulus 73.1 GPa against 3 GPa for Plastic Nylon PA66, so the same part in Aluminum 2024-T351 deflects less under the same load.

Which is lighter for the same job, Aluminum 2024-T351 or Plastic Nylon PA66?

For the same stiffness or strength: Aluminum 2024-T351 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie; Plastic Nylon PA66 is lighter for a strong panel or plate.

Part that must beAluminum 2024-T351Plastic Nylon PA66
Stiff rod or tie (tension)lighter9.94x heavier
Stiff beam (bending)lighter2.01x heavier
Stiff panel or platelighter18% heavier
Strong rod or tielighter1.55x heavier
Strong beamabout equalabout equal
Strong panel or plate26% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 2024-T351 or Plastic Nylon PA66?

Plastic Nylon PA66 stretches further before it breaks: 30% elongation at break against 19% for Aluminum 2024-T351.

Thermal

Which conducts heat better, Aluminum 2024-T351 or Plastic Nylon PA66?

Aluminum 2024-T351 conducts heat better: 120 W/m·K against 0.33 W/m·K for Plastic Nylon PA66.

Which expands less with temperature?

Aluminum 2024-T351 expands less: 22.9 µm/m·K against 98 µm/m·K for Plastic Nylon PA66.