Materials / Compare

Aluminum 2024-T351 vs. SLA Resin Tough 2000

Compare Aluminum 2024-T351 vs. SLA Resin Tough 2000 strength, stiffness, weight and thermal properties.

Aluminum 2024-T351Wrought
SLA Resin Tough 20003D printed (SLA resin)
MechanicalAluminum 2024-T351SLA Resin Tough 2000
Yield strength324MPa18.02x stronger40.4MPa2
Ultimate tensile strength469MPa111.6x stronger40.4MPa2
Flexural strengthnot sourced67MPa2
Elongation at break19%179%24.16x more ductile
Young's modulus (stiffness)73.1GPa140.6x stiffer1.8GPa2
Density2,770kg/m³11,090kg/m³22.54x lighter
Strength to weight117kN·m/kg3.16x higher37.1kN·m/kg
Stiffness to weight26.4MN·m/kg16x higher1.65MN·m/kg
Poisson's ratio0.333not sourced
Shear modulus27.5GPanot sourced
Bulk modulus71.7GPanot sourced
Speed of sound5,137m/s4x faster1,285m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 2024-T351SLA Resin Tough 2000
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 2024-T351SLA Resin Tough 2000
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 2024-T351SLA Resin Tough 2000
Thermal conductivity120W/m·K1not sourced
Thermal expansion22.9µm/m·K15.86x lessmean 0-150 °C134µm/m·K2
100 mm part over a 50 °C swing115µm growth5.86x less671µm growth
Specific heat875J/kg·K1not sourced
Heats up and cools (diffusivity)49.5mm²/snot sourced
Thermal shock resistance15,561W/mnot sourced
Melting pointmelting range502–638°C1not sourced
Glass transitionnot sourcedDMA112°C2
Max service temperaturenot sourcedHDT 1.8 MPa57°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 2024-T351
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 2024-T351
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Kaiser Aluminum, Formlabs, U.S. Department of Defense
Aluminum 2024-T351
2024-T4/T351, Kaiser Aluminum sheet, coil & plate typical datasheet; Poisson from MIL-HDBK-5J
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
  1. 1
    Alloy 2024 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 2024-T351 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 2024-T351 · Ultimate tensile strength: typicalAluminum 2024-T351 · Elongation at break: typical, in 4DAluminum 2024-T351 · Young's modulus (stiffness): typicalAluminum 2024-T351 · Density: nominalAluminum 2024-T351 · Thermal conductivity: typical, 20 °CAluminum 2024-T351 · Thermal expansion: typical, mean 20-100 °CAluminum 2024-T351 · Specific heat: typical, at 100 °CAluminum 2024-T351 · Melting point: melting range
  2. 2
    Tough 2000 Resin V2 Technical Data Sheet (2025)Formlabsarchived copySLA Resin Tough 2000 · Yield strength: typicalSLA Resin Tough 2000 · Ultimate tensile strength: typicalSLA Resin Tough 2000 · Flexural strength: typicalSLA Resin Tough 2000 · Elongation at break: typicalSLA Resin Tough 2000 · Young's modulus (stiffness): typicalSLA Resin Tough 2000 · Density: typicalSLA Resin Tough 2000 · Thermal expansion: mean 0-150 °CSLA Resin Tough 2000 · Glass transition: DMASLA Resin Tough 2000 · Max service temperature: HDT 1.8 MPa
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 2024-T351 · Poisson's ratio: typical (handbook physical constant), all tempers

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Aluminum 2024-T351 stronger than SLA Resin Tough 2000?

Aluminum 2024-T351 is stronger: its yield strength is 324 MPa against 40.4 MPa for SLA Resin Tough 2000 (8.02x).

Which is lighter, Aluminum 2024-T351 or SLA Resin Tough 2000?

SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 2,770 kg/m³ for Aluminum 2024-T351.

Which is stiffer, Aluminum 2024-T351 or SLA Resin Tough 2000?

Aluminum 2024-T351 is stiffer: Young's modulus 73.1 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Aluminum 2024-T351 deflects less under the same load.

Which is lighter for the same job, Aluminum 2024-T351 or SLA Resin Tough 2000?

For the same stiffness or strength: Aluminum 2024-T351 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 2024-T351SLA Resin Tough 2000
Stiff rod or tie (tension)lighter16x heavier
Stiff beam (bending)lighter2.51x heavier
Stiff panel or platelighter35% heavier
Strong rod or tielighter3.16x heavier
Strong beamlighter1.58x heavier
Strong panel or platelighter11% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 2024-T351 or SLA Resin Tough 2000?

SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 19% for Aluminum 2024-T351.

Thermal

Which expands less with temperature?

Aluminum 2024-T351 expands less: 22.9 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.