Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Sources5 documents: Kaiser Aluminum, American Institute of Steel Construction, bauforumstahl (ArcelorMittal), Ovako
Aluminum 3003-O
3003-O (annealed) aluminium-manganese alloy, the heat-exchanger tube and brazing alloy, Kaiser Aluminum Tube & Pipe Alloy 3003 Technical Data (Rev. 05/06), typical properties; specific heat from the NIST cryogenic 3003-F fit at 293 K.
Steel
Generic structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.
1
Alloy 3003 Tube & Pipe Technical Data, Rev. 05/06Kaiser Aluminumarchived copyAluminum 3003-O · Yield strength: typical, O, 0.0625 in specimenAluminum 3003-O · Ultimate tensile strength: typical, OAluminum 3003-O · Elongation at break: typical, O, in 4DAluminum 3003-O · Young's modulus (stiffness): typicalAluminum 3003-O · Density: nominal, 20 °CAluminum 3003-O · Thermal conductivity: typical, O, 20 °CAluminum 3003-O · Thermal expansion: typical, mean 20-100 °CAluminum 3003-O · Melting point: melting range
2
Updating Standard Shape Material Properties Database for Design and ReliabilityAmerican Institute of Steel Constructionarchived copySteel · Yield strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISCSteel · Ultimate tensile strength: typical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)Steel · Elongation at break: typical: mean of 24,847 A992 mill-test elongations, web and flange (1998 SSPC mill data), as reported by AISC
3
ANSI/AISC 360-16 Specification for Structural Steel Buildings, with CommentaryAmerican Institute of Steel Constructionarchived copySteel · Young's modulus (stiffness): design value (AISC 360-16)Steel · Poisson's ratio: design value (AISC 360-16 Commentary)
4
Environmental Product Declaration: Structural Steel Sections and Merchant Bars (2023)bauforumstahl (ArcelorMittal)archived copySteel · Density: nominal (constructional data)Steel · Thermal conductivity: nominal at 20 °CSteel · Thermal expansion: nominal (constructional data, no temperature range stated)
5
S275JR Steel GradeOvakoSteel · Specific heat: base material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 3003-O stronger than Steel?
Steel is stronger: its yield strength is 385 MPa against 40 MPa for Aluminum 3003-O (9.63x).
Which is lighter, Aluminum 3003-O or Steel?
Aluminum 3003-O is lighter: 2,730 kg/m³ against 7,850 kg/m³ for Steel.
Which is stiffer, Aluminum 3003-O or Steel?
Steel is stiffer: Young's modulus 200 GPa against 69 GPa for Aluminum 3003-O, so the same part in Steel deflects less under the same load.
Which is lighter for the same job, Aluminum 3003-O or Steel?
For the same stiffness or strength: Aluminum 3003-O is lighter for a stiff beam (bending), stiff panel or plate; Steel is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 3003-O
Steel
Stiff rod or tie (tension)
about equal
about equal
Stiff beam (bending)
lighter
1.69x heavier
Stiff panel or plate
lighter
2.02x heavier
Strong rod or tie
3.35x heavier
lighter
Strong beam
1.57x heavier
lighter
Strong panel or plate
8% heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 3003-O or Steel?
Aluminum 3003-O stretches further before it breaks: 30% elongation at break against 24.2% for Steel.
Thermal
Which conducts heat better, Aluminum 3003-O or Steel?
Aluminum 3003-O conducts heat better: 193 W/m·K against 48 W/m·K for Steel.
Which expands less with temperature?
Steel expands less: 12 µm/m·K against 23.2 µm/m·K for Aluminum 3003-O.