Materials / Compare
Aluminum 5052-H32 vs. DMLS 17-4PH Stainless Steel
Compare Aluminum 5052-H32 vs. DMLS 17-4PH Stainless Steel strength, stiffness, weight and thermal properties.
| Mechanical | Aluminum 5052-H32 | DMLS 17-4PH Stainless Steel |
|---|---|---|
| Yield strength | 195MPa1 | mean861MPa24.41x stronger |
| Ultimate tensile strength | 230MPa1 | mean886MPa23.85x stronger |
| Elongation at break | 12%1 | mean at break19.9%21.66x more ductile |
| Young's modulus (stiffness) | 70GPa1 | base material197GPa32.81x stiffer |
| Density | 2,685kg/m³42.9x lighter | mean part density7,790kg/m³2 |
| Strength to weight | 72.6kN·m/kg | 110kN·m/kg1.52x higher |
| Stiffness to weight | 26.1MN·m/kg3% higher | 25.3MN·m/kg |
| Poisson's ratio | 0.334 | base material0.2723 |
| Shear modulus | 26.3GPa | 77.4GPa2.94x stiffer in shear |
| Bulk modulus | 68.6GPa | 144GPa2.1x higher |
| Speed of sound | 5,106m/s2% faster | 5,029m/s |
| Thermal | Aluminum 5052-H32 | DMLS 17-4PH Stainless Steel |
|---|---|---|
| Thermal conductivity | base material138W/m·K17.71x more heat through a fin | base material17.9W/m·K3 |
| Thermal expansion | 23.8µm/m·K1 | mean 25-100 °C10.4µm/m·K22.29x less |
| 100 mm part over a 50 °C swing | 119µm growth | 52µm growth2.29x less |
| Specific heat | at 100 °C963J/kg·K42.09x higher | base material460J/kg·K3 |
| Heats up and cools (diffusivity) | 53.4mm²/s10.7x faster | 5mm²/s |
| Thermal shock resistance | 10,822W/m1.98x more resistant | 5,474W/m |
| Melting point | melting range605–650°C1 | not sourced |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources4 documents: Kaiser Aluminum, EOS GmbH, Cleveland-Cliffs, U.S. Department of Defense
- Aluminum 5052-H32
- 5052-H32, Kaiser Aluminum tube & pipe typical datasheet (mechanical, CTE, melting); MIL-HDBK-5J (Poisson, density, specific heat)
- DMLS 17-4PH Stainless Steel
- EOS StainlessSteel 17-4PH IndustryLine (powder 9011-0041), EOS M 290, 40 µm, default job 17-4PH_040_StainlessM291_100, as built, horizontal; ISO 6892 & ASTM E8M
- 1Alloy 5052 Tube & Pipe Technical DataKaiser Aluminumarchived copyAluminum 5052-H32 · Yield strength: typical, 0.2% offsetAluminum 5052-H32 · Ultimate tensile strength: typicalAluminum 5052-H32 · Elongation at break: typicalAluminum 5052-H32 · Young's modulus (stiffness): typicalAluminum 5052-H32 · Thermal conductivity: base material: 5052 in O temper (same alloy, annealed); Kaiser typicalAluminum 5052-H32 · Thermal expansion: typical, mean 20-100 °CAluminum 5052-H32 · Melting point: melting range
- 2EOS StainlessSteel 17-4PH IndustryLine Material Data Sheet, M 290EOS GmbHarchived copyDMLS 17-4PH Stainless Steel · Yield strength: mean, as built, horizontal (N=72)DMLS 17-4PH Stainless Steel · Ultimate tensile strength: mean, as built, horizontal (N=72)DMLS 17-4PH Stainless Steel · Elongation at break: mean at break, as built, horizontalDMLS 17-4PH Stainless Steel · Density: mean part density (ISO 3369)DMLS 17-4PH Stainless Steel · Thermal expansion: mean 25-100 °C, ASTM E228, AFTER atmospheric heat treatment (as-built value not published)
- 317-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsDMLS 17-4PH Stainless Steel · Young's modulus (stiffness): base material: wrought 17-4 PH, Condition H 900 (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Poisson's ratio: base material: wrought 17-4 PH, all conditions (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Thermal conductivity: base material: wrought 17-4 PH, Condition H 900, at 149 °C (Cleveland-Cliffs)DMLS 17-4PH Stainless Steel · Specific heat: base material: wrought 17-4 PH, Condition A, 0-100 °C (Cleveland-Cliffs)
- 4MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 5052-H32 · Density: nominalAluminum 5052-H32 · Poisson's ratio: typical (handbook physical constant)Aluminum 5052-H32 · Specific heat: at 100 °C (212 °F); table covers O, H32, H34, H36, H38
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS 17-4PH Stainless Steel is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 5052-H32 stronger than DMLS 17-4PH Stainless Steel?
DMLS 17-4PH Stainless Steel is stronger: its yield strength is 861 MPa against 195 MPa for Aluminum 5052-H32 (4.41x).
Which is lighter, Aluminum 5052-H32 or DMLS 17-4PH Stainless Steel?
Aluminum 5052-H32 is lighter: 2,685 kg/m³ against 7,790 kg/m³ for DMLS 17-4PH Stainless Steel.
Which is stiffer, Aluminum 5052-H32 or DMLS 17-4PH Stainless Steel?
DMLS 17-4PH Stainless Steel is stiffer: Young's modulus 197 GPa against 70 GPa for Aluminum 5052-H32, so the same part in DMLS 17-4PH Stainless Steel deflects less under the same load.
Which is lighter for the same job, Aluminum 5052-H32 or DMLS 17-4PH Stainless Steel?
For the same stiffness or strength: Aluminum 5052-H32 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong beam, strong panel or plate; DMLS 17-4PH Stainless Steel is lighter for a strong rod or tie.
| Part that must be | Aluminum 5052-H32 | DMLS 17-4PH Stainless Steel |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 3% heavier |
| Stiff beam (bending) | lighter | 1.73x heavier |
| Stiff panel or plate | lighter | 2.05x heavier |
| Strong rod or tie | 1.52x heavier | lighter |
| Strong beam | lighter | 8% heavier |
| Strong panel or plate | lighter | 38% heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 5052-H32 or DMLS 17-4PH Stainless Steel?
DMLS 17-4PH Stainless Steel stretches further before it breaks: 19.9% elongation at break against 12% for Aluminum 5052-H32.
Thermal
Which conducts heat better, Aluminum 5052-H32 or DMLS 17-4PH Stainless Steel?
Aluminum 5052-H32 conducts heat better: 138 W/m·K against 17.9 W/m·K for DMLS 17-4PH Stainless Steel.
Which expands less with temperature?
DMLS 17-4PH Stainless Steel expands less: 10.4 µm/m·K against 23.8 µm/m·K for Aluminum 5052-H32.
Related comparisons
- Aluminum 5052-H32 vs. Aluminum 6063-T6
- Aluminum 5052-H32 vs. Aluminum A380
- Aluminum 5052-H32 vs. Aluminum ADC12
- Aluminum 5052-H32 vs. DMLS AlSi10Mg Aluminum
- DMLS 17-4PH Stainless Steel vs. Steel AISI 4340
- DMLS 17-4PH Stainless Steel vs. Nickel Inconel 718
- DMLS 17-4PH Stainless Steel vs. Stainless Steel 17-4PH
- DMLS 17-4PH Stainless Steel vs. Steel AISI 1045