Materials / Compare
Aluminum 5052-H32 vs. DMLS 316L Stainless Steel
Compare Aluminum 5052-H32 vs. DMLS 316L Stainless Steel strength, stiffness, weight and thermal properties.
| Mechanical | Aluminum 5052-H32 | DMLS 316L Stainless Steel |
|---|---|---|
| Yield strength | 195MPa1 | 530MPa22.72x stronger |
| Ultimate tensile strength | 230MPa1 | 640MPa22.78x stronger |
| Elongation at break | 12%1 | 40%23.33x more ductile |
| Young's modulus (stiffness) | 70GPa1 | 185GPa32.64x stiffer |
| Density | 2,685kg/m³42.94x lighter | part density7,900kg/m³5 |
| Strength to weight | 72.6kN·m/kg8% higher | 67.1kN·m/kg |
| Stiffness to weight | 26.1MN·m/kg11% higher | 23.4MN·m/kg |
| Poisson's ratio | 0.334 | base material0.36 |
| Shear modulus | 26.3GPa | 71.2GPa2.7x stiffer in shear |
| Bulk modulus | 68.6GPa | 154GPa2.25x higher |
| Speed of sound | 5,106m/s6% faster | 4,839m/s |
| Thermal | Aluminum 5052-H32 | DMLS 316L Stainless Steel |
|---|---|---|
| Thermal conductivity | base material138W/m·K18.52x more heat through a fin | base material16.2W/m·K7 |
| Thermal expansion | 23.8µm/m·K1 | mean 25-100 °C15.7µm/m·K21.51x less |
| 100 mm part over a 50 °C swing | 119µm growth | 78.6µm growth1.51x less |
| Specific heat | at 100 °C963J/kg·K41.93x higher | base material500J/kg·K7 |
| Heats up and cools (diffusivity) | 53.4mm²/s13x faster | 4.1mm²/s |
| Thermal shock resistance | 10,822W/m5.24x more resistant | 2,067W/m |
| Melting point | melting range605–650°C1 | not sourced |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources7 documents: Kaiser Aluminum, EOS GmbH, U.S. Department of Defense, Steel Construction Institute, Cleveland-Cliffs
- Aluminum 5052-H32
- 5052-H32, Kaiser Aluminum tube & pipe typical datasheet (mechanical, CTE, melting); MIL-HDBK-5J (Poisson, density, specific heat)
- DMLS 316L Stainless Steel
- EOS StainlessSteel 316L (powder 9011-0032), EOS M 290, ParameterSet 316L 20µm Surface M290/400W, as manufactured, horizontal; ISO 6892-1
- 1Alloy 5052 Tube & Pipe Technical DataKaiser Aluminumarchived copyAluminum 5052-H32 · Yield strength: typical, 0.2% offsetAluminum 5052-H32 · Ultimate tensile strength: typicalAluminum 5052-H32 · Elongation at break: typicalAluminum 5052-H32 · Young's modulus (stiffness): typicalAluminum 5052-H32 · Thermal conductivity: base material: 5052 in O temper (same alloy, annealed); Kaiser typicalAluminum 5052-H32 · Thermal expansion: typical, mean 20-100 °CAluminum 5052-H32 · Melting point: melting range
- 2EOS StainlessSteel 316L Material Data SheetEOS GmbHarchived copyDMLS 316L Stainless Steel · Yield strength: typical, as manufactured, horizontalDMLS 316L Stainless Steel · Ultimate tensile strength: typical, as manufactured, horizontalDMLS 316L Stainless Steel · Elongation at break: typical at break, as manufactured, horizontalDMLS 316L Stainless Steel · Thermal expansion: mean 25-100 °C, ASTM E228
- 3EOS StainlessSteel 316L Material Data Sheet, M 280 and M 290 (2014)EOS GmbHarchived copyDMLS 316L Stainless Steel · Young's modulus (stiffness): typical, as built, horizontal (XY); EOSINT M280-400W / M290-400W, 316L_Surface 1.0, 20 µm (2014 sheet)
- 4MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 5052-H32 · Density: nominalAluminum 5052-H32 · Poisson's ratio: typical (handbook physical constant)Aluminum 5052-H32 · Specific heat: at 100 °C (212 °F); table covers O, H32, H34, H36, H38
- 5EOS StainlessSteel 316L Material Data Sheet, FlexLine, M 290 (2016)EOS GmbHarchived copyDMLS 316L Stainless Steel · Density: part density (ISO 3369, not labelled min or typical), EOS M 290, 40 µm FlexLine
- 6Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyDMLS 316L Stainless Steel · Poisson's ratio: base material: austenitic stainless steels incl. 1.4404 (316L), design value
- 7316/316L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsDMLS 316L Stainless Steel · Thermal conductivity: base material: wrought 316/316L (Cleveland-Cliffs), at 100 °CDMLS 316L Stainless Steel · Specific heat: base material: wrought 316/316L (Cleveland-Cliffs), 0-100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS 316L Stainless Steel is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 5052-H32 stronger than DMLS 316L Stainless Steel?
DMLS 316L Stainless Steel is stronger: its yield strength is 530 MPa against 195 MPa for Aluminum 5052-H32 (2.72x).
Which is lighter, Aluminum 5052-H32 or DMLS 316L Stainless Steel?
Aluminum 5052-H32 is lighter: 2,685 kg/m³ against 7,900 kg/m³ for DMLS 316L Stainless Steel.
Which is stiffer, Aluminum 5052-H32 or DMLS 316L Stainless Steel?
DMLS 316L Stainless Steel is stiffer: Young's modulus 185 GPa against 70 GPa for Aluminum 5052-H32, so the same part in DMLS 316L Stainless Steel deflects less under the same load.
Which is lighter for the same job, Aluminum 5052-H32 or DMLS 316L Stainless Steel?
For the same stiffness or strength: Aluminum 5052-H32 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
| Part that must be | Aluminum 5052-H32 | DMLS 316L Stainless Steel |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 11% heavier |
| Stiff beam (bending) | lighter | 1.81x heavier |
| Stiff panel or plate | lighter | 2.13x heavier |
| Strong rod or tie | lighter | 8% heavier |
| Strong beam | lighter | 1.51x heavier |
| Strong panel or plate | lighter | 1.78x heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 5052-H32 or DMLS 316L Stainless Steel?
DMLS 316L Stainless Steel stretches further before it breaks: 40% elongation at break against 12% for Aluminum 5052-H32.
Thermal
Which conducts heat better, Aluminum 5052-H32 or DMLS 316L Stainless Steel?
Aluminum 5052-H32 conducts heat better: 138 W/m·K against 16.2 W/m·K for DMLS 316L Stainless Steel.
Which expands less with temperature?
DMLS 316L Stainless Steel expands less: 15.7 µm/m·K against 23.8 µm/m·K for Aluminum 5052-H32.
Related comparisons
- Aluminum 5052-H32 vs. Aluminum 6063-T6
- Aluminum 5052-H32 vs. Aluminum A380
- Aluminum 5052-H32 vs. Aluminum ADC12
- Aluminum 5052-H32 vs. DMLS AlSi10Mg Aluminum
- DMLS 316L Stainless Steel vs. Steel AISI 1045
- DMLS 316L Stainless Steel vs. Steel
- DMLS 316L Stainless Steel vs. Steel A992
- DMLS 316L Stainless Steel vs. Steel AISI 1018