Materials / Compare

Aluminum 5052-H32 vs. Plastic PMMA

Compare Aluminum 5052-H32 vs. Plastic PMMA strength, stiffness, weight and thermal properties.

Aluminum 5052-H32Wrought
Plastic PMMABulk polymer (molded or machined)
MechanicalAluminum 5052-H32Plastic PMMA
Yield strength195MPa1not given (tensile used)
Ultimate tensile strength230MPa12.88x stronger80MPa2
Compressive strengthnot sourced110MPa2
Flexural strengthnot sourced115MPa2
Elongation at break12%12.18x more ductile5.5%2
Young's modulus (stiffness)70GPa121.2x stiffer3.3GPa2
Density2,685kg/m³31,190kg/m³22.26x lighter
Strength to weight72.6kN·m/kg8% higher67.2kN·m/kg
Stiffness to weight26.1MN·m/kg9.4x higher2.77MN·m/kg
Poisson's ratio0.3330.372
Shear modulus26.3GPa21.9x stiffer in shear1.2GPa
Bulk modulus68.6GPa16.2x higher4.23GPa
Speed of sound5,106m/s3.07x faster1,665m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 5052-H32Plastic PMMA
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 5052-H32Plastic PMMA
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 5052-H32Plastic PMMA
Thermal conductivitybase material138W/m·K1726x more heat through a fin0.19W/m·K2
Thermal expansion23.8µm/m·K12.94x less0-50 °C70µm/m·K2
100 mm part over a 50 °C swing119µm growth2.94x less350µm growth
Specific heatat 100 °C963J/kg·K31,470J/kg·K21.53x higher
Heats up and cools (diffusivity)53.4mm²/s491x faster0.109mm²/s
Thermal shock resistance10,822W/m261x more resistant41.5W/m
Melting pointmelting range605–650°C1not sourced
Max service temperaturenot sourced80°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 5052-H32Plastic PMMA
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 5052-H32Plastic PMMA
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Kaiser Aluminum, Röhm, U.S. Department of Defense
Aluminum 5052-H32
5052-H32, Kaiser Aluminum tube & pipe typical datasheet (mechanical, CTE, melting); MIL-HDBK-5J (Poisson, density, specific heat)
Plastic PMMA
Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)
  1. 1
    Alloy 5052 Tube & Pipe Technical DataKaiser Aluminumarchived copyAluminum 5052-H32 · Yield strength: typical, 0.2% offsetAluminum 5052-H32 · Ultimate tensile strength: typicalAluminum 5052-H32 · Elongation at break: typicalAluminum 5052-H32 · Young's modulus (stiffness): typicalAluminum 5052-H32 · Thermal conductivity: base material: 5052 in O temper (same alloy, annealed); Kaiser typicalAluminum 5052-H32 · Thermal expansion: typical, mean 20-100 °CAluminum 5052-H32 · Melting point: melting range
  2. 2
    PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 5052-H32 · Density: nominalAluminum 5052-H32 · Poisson's ratio: typical (handbook physical constant)Aluminum 5052-H32 · Specific heat: at 100 °C (212 °F); table covers O, H32, H34, H36, H38

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 5052-H32 stronger than Plastic PMMA?

Aluminum 5052-H32 is stronger: its yield strength is 195 MPa against tensile strength 80 MPa for Plastic PMMA (2.44x).

Which is lighter, Aluminum 5052-H32 or Plastic PMMA?

Plastic PMMA is lighter: 1,190 kg/m³ against 2,685 kg/m³ for Aluminum 5052-H32.

Which is stiffer, Aluminum 5052-H32 or Plastic PMMA?

Aluminum 5052-H32 is stiffer: Young's modulus 70 GPa against 3.3 GPa for Plastic PMMA, so the same part in Aluminum 5052-H32 deflects less under the same load.

Which is lighter for the same job, Aluminum 5052-H32 or Plastic PMMA?

For the same stiffness or strength: Aluminum 5052-H32 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie; Plastic PMMA is lighter for a strong beam, strong panel or plate.

Part that must beAluminum 5052-H32Plastic PMMA
Stiff rod or tie (tension)lighter9.4x heavier
Stiff beam (bending)lighter2.04x heavier
Stiff panel or platelighter23% heavier
Strong rod or tielighter8% heavier
Strong beam25% heavierlighter
Strong panel or plate45% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 5052-H32 or Plastic PMMA?

Aluminum 5052-H32 stretches further before it breaks: 12% elongation at break against 5.5% for Plastic PMMA.

Thermal

Which conducts heat better, Aluminum 5052-H32 or Plastic PMMA?

Aluminum 5052-H32 conducts heat better: 138 W/m·K against 0.19 W/m·K for Plastic PMMA.

Which expands less with temperature?

Aluminum 5052-H32 expands less: 23.8 µm/m·K against 70 µm/m·K for Plastic PMMA.