Materials / Compare

Aluminum 6061-T6 vs. DMLS AlSi10Mg Aluminum

Compare Aluminum 6061-T6 vs. DMLS AlSi10Mg Aluminum strength, stiffness, weight and thermal properties.

Change either side
Aluminum 6061-T6Wrought
DMLS AlSi10Mg Aluminum3D printed metal (DMLS)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength276MPasourcetypical, 0.2% offset, .500 in dia specimen270MPasourcetypical, as manufactured, horizontal
Ultimate tensile strength310MPasourcetypical450MPasourcetypical, as manufactured, horizontal
Elongation at break17%sourcetypical, in 4D, 0.500 in dia specimen10.2%sourcetypical at break, as manufactured, horizontal
Young's modulus (stiffness)68.3GPasourcetypical72GPasourcesame material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
Density2,700kg/m³sourcenominal2,670kg/m³sourcetypical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
Strength to weight102kN·m/kg1% higher101kN·m/kg
Stiffness to weight25.3MN·m/kg27MN·m/kg7% higher
Poisson's ratio0.33sourcetypical (handbook physical constant)0.33sourcebase material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)
Shear modulus25.7GPa27.1GPa5% stiffer in shear
Bulk modulus67GPa70.6GPa
Speed of sound5,030m/s5,193m/s
Thermal
Thermal conductivity167W/m·Ksourcetypical, 20 °C110W/m·Ksourcetypical, as manufactured, horizontal (ISO 22007-2)
Thermal expansion23.6µm/m·Ksourcetypical, mean 20-100 °C20µm/m·Ksourcemean 25-100 °C, ASTM E228
100 mm part over a 50 °C swing118µm growth100µm growth18% less
Specific heat896J/kg·Ksourcetypical, at 100 °C963J/kg·Ksourcebase material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
Heats up and cools (diffusivity)69mm²/s1.61x faster42.8mm²/s
Thermal shock resistance19,159W/m39% more resistant13,819W/m
Melting point582–652°Csourcesolidus-liquidusnot sourced
Values for6061-T6/T651, Kaiser Aluminum typical properties; Poisson from MIL-HDBK-5JEOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Aluminum 6061-T6 stronger than DMLS AlSi10Mg Aluminum?

Aluminum 6061-T6 is stronger: its yield strength is 276 MPa against 270 MPa for DMLS AlSi10Mg Aluminum (2%).

Which is lighter, Aluminum 6061-T6 or DMLS AlSi10Mg Aluminum?

DMLS AlSi10Mg Aluminum is lighter: 2,670 kg/m³ against 2,700 kg/m³ for Aluminum 6061-T6.

Which is stiffer, Aluminum 6061-T6 or DMLS AlSi10Mg Aluminum?

DMLS AlSi10Mg Aluminum is stiffer: Young's modulus 72 GPa against 68.3 GPa for Aluminum 6061-T6, so the same part in DMLS AlSi10Mg Aluminum deflects less under the same load.

Which is lighter for the same job, Aluminum 6061-T6 or DMLS AlSi10Mg Aluminum?

For the same stiffness or strength: Aluminum 6061-T6 is lighter for a strong rod or tie; DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beAluminum 6061-T6DMLS AlSi10Mg Aluminum
Stiff rod or tie (tension)7% heavierlighter
Stiff beam (bending)4% heavierlighter
Stiff panel or plate3% heavierlighter
Strong rod or tielighter1% heavier
Strong beamabout equalabout equal
Strong panel or plateabout equalabout equal

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum 6061-T6 or DMLS AlSi10Mg Aluminum?

Aluminum 6061-T6 conducts heat better: 167 W/m·K against 110 W/m·K for DMLS AlSi10Mg Aluminum.

Which expands less with temperature?

DMLS AlSi10Mg Aluminum expands less: 20 µm/m·K against 23.6 µm/m·K for Aluminum 6061-T6.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 6061-T6DMLS AlSi10Mg Aluminum
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 6061-T6DMLS AlSi10Mg Aluminum
Strength against density

Related comparisons