Materials / Compare
Aluminum 6063-T6 vs. DMLS AlSi10Mg Aluminum
Compare Aluminum 6063-T6 vs. DMLS AlSi10Mg Aluminum strength, stiffness, weight and thermal properties.
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|---|---|
| Mechanical | ||
| Yield strength | 215MPasourcetypical, T6, 0.0625 in specimen | 270MPasourcetypical, as manufactured, horizontal |
| Ultimate tensile strength | 240MPasourcetypical, T6 | 450MPasourcetypical, as manufactured, horizontal |
| Elongation at break | 12%sourcetypical, T6, in 4D | 10.2%sourcetypical at break, as manufactured, horizontal |
| Young's modulus (stiffness) | 69GPasourcetypical | 72GPasourcesame material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY) |
| Density | 2,700kg/m³sourcenominal, 20 °C | 2,670kg/m³sourcetypical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm) |
| Strength to weight | 79.6kN·m/kg | 101kN·m/kg27% higher |
| Stiffness to weight | 25.6MN·m/kg | 27MN·m/kg6% higher |
| Poisson's ratio | not sourced | 0.33sourcebase material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000) |
| Shear modulus | not sourced | 27.1GPa |
| Bulk modulus | not sourced | 70.6GPa |
| Speed of sound | 5,055m/s | 5,193m/s |
| Thermal | ||
| Thermal conductivity | 201W/m·Ksourcetypical, T6, 20 °C | 110W/m·Ksourcetypical, as manufactured, horizontal (ISO 22007-2) |
| Thermal expansion | 23.4µm/m·Ksourcetypical, mean 20-100 °C | 20µm/m·Ksourcemean 25-100 °C, ASTM E228 |
| 100 mm part over a 50 °C swing | 117µm growth | 100µm growth17% less |
| Specific heat | 901J/kg·Ksourcetypical, 20 °C (Hydro EN AW-6063) | 963J/kg·Ksourcebase material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C |
| Heats up and cools (diffusivity) | 82.6mm²/s1.93x faster | 42.8mm²/s |
| Thermal shock resistance | not sourced | 13,819W/m |
| Melting point | 615–655°Csourcemelting range | not sourced |
| Values for | 6063-T6 extruded tube, Kaiser Aluminum Tube & Pipe Alloy 6063 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-6063 extruded-products datasheet (Rev.4, 03/2023). | EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10 |
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Is Aluminum 6063-T6 stronger than DMLS AlSi10Mg Aluminum?
DMLS AlSi10Mg Aluminum is stronger: its yield strength is 270 MPa against 215 MPa for Aluminum 6063-T6 (26%).
Which is lighter, Aluminum 6063-T6 or DMLS AlSi10Mg Aluminum?
DMLS AlSi10Mg Aluminum is lighter: 2,670 kg/m³ against 2,700 kg/m³ for Aluminum 6063-T6.
Which is stiffer, Aluminum 6063-T6 or DMLS AlSi10Mg Aluminum?
DMLS AlSi10Mg Aluminum is stiffer: Young's modulus 72 GPa against 69 GPa for Aluminum 6063-T6, so the same part in DMLS AlSi10Mg Aluminum deflects less under the same load.
Which is lighter for the same job, Aluminum 6063-T6 or DMLS AlSi10Mg Aluminum?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
| Part that must be | Aluminum 6063-T6 | DMLS AlSi10Mg Aluminum |
|---|---|---|
| Stiff rod or tie (tension) | 6% heavier | lighter |
| Stiff beam (bending) | 3% heavier | lighter |
| Stiff panel or plate | 3% heavier | lighter |
| Strong rod or tie | 27% heavier | lighter |
| Strong beam | 18% heavier | lighter |
| Strong panel or plate | 13% heavier | lighter |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which conducts heat better, Aluminum 6063-T6 or DMLS AlSi10Mg Aluminum?
Aluminum 6063-T6 conducts heat better: 201 W/m·K against 110 W/m·K for DMLS AlSi10Mg Aluminum.
Which expands less with temperature?
DMLS AlSi10Mg Aluminum expands less: 20 µm/m·K against 23.4 µm/m·K for Aluminum 6063-T6.